MP 54460
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Multi-Substrate Structural Adhesion
- Documented Water/Salt-Spray/Acid/Solvent Resistance
- 3 to 5-Minute Handling Time
Product Description
MP5405 is a clear, two-part unfilled epoxy structural adhesive designed for bonding ceramics, metals, and most plastics. It features a 1:1 mix ratio and cures at room temperature to form a tough, semi-rigid material that offers strong resistance to water, salt spray, and various chemicals.
Key features
- Fast handling strength: Achieves handling strength in 3 to 5 minutes at room temperature for quick assembly.
- Excellent chemical resistance: Withstands water, salt spray, inorganic acids and bases, and most organic solvents.
- Convenient 1:1 mix ratio: Easily dispensed using either static mixing nozzles in dual cartridges or MMD equipment.
Applications / Suitable for
- Designed for bonding ceramics, metals, and most plastics.
- Suitable for use in either MMD equipment or side-by-side dual cartridges.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
Pre-cure properties of MP5405 epoxy adhesive.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance / Color | Clear | - | - |
| Mix Ratio (Volume & Weight) | 1:1 | - | - |
| Viscosity (Mixed) | 12,500 | cPs | at 25°C |
| Specific Gravity (Mixed) | 1.16 | - | - |
| Pot Life | 3 to 5 | min | at 25°C, 20 gram |
After-processing / final-state properties
Cured mechanical and electrical properties of MP5405 after full cure.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Hardness | 80 | Shore D | ASTM D2240 |
| Tensile Strength | 48.3 (7000) | MPa (psi) | ASTM D638 |
| Overlap Shear Strength | 15.9 (2300) | MPa (psi) | Aluminum, Acid Etched, 25°C, ASTM D1002 |
| Operating Temperature | -40 to 130 | °C | - |
| Dielectric Strength | 16.1 | kV/mm | ASTM D149 |