PERMABOND 102
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Low 70–90 mPa·s viscosity
- 0.15 mm maximum gap fill
- Typical fixture times of 5–15 seconds
Product Description
PERMABOND® 102 Cyanoacrylate Adhesive is a low-viscosity, single-component ethyl cyanoacrylate adhesive designed for fast bonding of close-fitting components. According to the TDS, its 70–90 mPa·s viscosity supports controlled flow into small bond gaps while maintaining rapid fixture performance. It is suitable for plastics, rubber, and metals, with a maximum recommended gap fill of 0.15 mm. Depending on the substrate, handling strength is typically reached within 5–15 seconds, while full strength develops in approximately 24 hours. The cured adhesive provides high shear strength on metals and selected plastics together with electrical insulating properties suitable for general industrial assembly.
Key features
- Low-viscosity formulation: A TDS viscosity of 70–90 mPa·s supports bonding of close-fitting components and narrow joints.
- Fast fixture performance: Typical handling strength is achieved in approximately 5–15 seconds depending on substrate.
- Multi-material bonding: Documented performance includes steel, aluminum, zinc, ABS, PVC, polycarbonate, phenolic, and Buna N rubber.
Applications / Suitable for
- Close-fitting component assembly
- Plastic and rubber bonding
- Metal bonding
- High-speed production and fast-fixturing applications
- Small-gap joints up to 0.15 mm
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Curing Conditions
Mechanical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical uncured and curing properties from the product technical datasheet. Values are guideline information and do not constitute product specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical composition | Ethyl cyanoacrylate | — | Single-component adhesive |
| Appearance | Colorless | — | As supplied |
| Viscosity | 70–90 | mPa·s | At 25 °C; TDS value; equivalent to cP |
| Specific gravity | 1.1 | — | Typical uncured value |
| Maximum gap fill | 0.15 | mm | Equivalent source value 0.006 in |
| Fixture time — steel | 10–15 | s | Time to 0.3 N/mm² shear strength |
| Fixture time — Buna N rubber | 5–10 | s | Time to 0.3 N/mm² shear strength |
| Fixture time — phenolic | 10–15 | s | Time to 0.3 N/mm² shear strength |
| Fixture time — PVC | 7–10 | s | Time to 0.3 N/mm² shear strength |
| Fixture time — ABS | 7–10 | s | Time to 0.3 N/mm² shear strength |
| Full strength | 24 | h | Typical full-strength development |
After-processing / final-state properties
Typical cured performance values from the TDS. Bond strength varies with substrate, surface preparation, bond gap, and curing conditions.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shear strength — steel | 19–23 | N/mm² | ISO 4587; equivalent source range 2,800–3,300 psi |
| Shear strength — aluminum | 7–9 | N/mm² | ISO 4587; equivalent source range 1,000–1,300 psi |
| Shear strength — zinc | 8–10 | N/mm² | ISO 4587; equivalent source range 1,200–1,500 psi |
| Shear strength — ABS | >6 | N/mm² | ISO 4587; substrate failure reported |
| Shear strength — PVC | >6 | N/mm² | ISO 4587; substrate failure reported |
| Shear strength — polycarbonate | >5 | N/mm² | ISO 4587; substrate failure reported |
| Shear strength — phenolic | 12–14 | N/mm² | ISO 4587; equivalent source range 1,700–2,000 psi |
| Impact strength | 3–5 | kJ/m² | ASTM D950 |
| Hardness | 85 | Shore D | ISO 868 |
| Dielectric constant | 2.5 | — | At 10 kHz |
| Dielectric strength | 25 | kV/mm | Typical cured electrical property |
| Coefficient of thermal expansion | 90 × 10-6 | mm/mm/°C | Typical cured thermal property |
| Thermal conductivity | 0.1 | W/(m·K) | Typical cured thermal property |
| Minimum exposure temperature | -55 | °C | Depends on bonded materials; equivalent source value -65 °F |