PERMABOND 200
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- 1,500 mPa s Application Viscosity
- 15-Second Fixturing Time
- 22 N/mm^2 Shear Strength
Product Description
PERMABOND® 200 Cyanoacrylate Adhesive is a high-viscosity, single-component ethyl cyanoacrylate adhesive developed for wire-tacking and general component-bonding applications. Its 1,500 mPa·s viscosity supports controlled placement and helps bridge gaps up to 0.38 mm. The adhesive is suitable for plastics, rubber, and metals and reaches typical handling strength in approximately 15 seconds on steel, Buna N rubber, and phenolic. Full strength develops in 24 hours. The solvent-free, 100% reactive formulation requires no mixing or heat cure and is suited to rapid industrial assembly.
Key features
- High-viscosity formulation: A viscosity of 1,500 mPa·s supports controlled application, wire tacking, and gap filling up to 0.38 mm.
- Fast fixture performance: Reaches typical handling strength in approximately 15 seconds on steel, Buna N rubber, and phenolic.
- Simple one-part processing: Requires no mixing or heat cure and contains no solvent.
Applications / Suitable for
- Wire-tacking applications
- Bonding components with small gaps
- High-speed industrial assembly
- Bonding plastics, rubber, and metals
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical uncured and curing properties. Values are guideline information and do not constitute product specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical composition | Ethyl cyanoacrylate | — | Single-component adhesive |
| Appearance | Colorless liquid | — | As supplied |
| Viscosity | 1,500 | mPa·s | At 25 °C; equivalent to cP |
| Specific gravity | 1.05 | — | Typical uncured value |
| Maximum gap fill | 0.38 | mm | Equivalent source value 0.015 in |
| Fixture time — steel | 15 | s | Time to 0.3 N/mm² shear strength |
| Fixture time — Buna N rubber | 15 | s | Time to 0.3 N/mm² shear strength |
| Fixture time — phenolic | 15 | s | Time to 0.3 N/mm² shear strength |
| Full strength | 24 | h | Typical full-strength development |
After-processing / final-state properties
Typical cured performance values. Bond strength varies with substrate, surface preparation, joint gap, and curing conditions.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shear strength — steel | 22 | N/mm² | ISO 4587; equivalent source value 3,200 psi |
| Shear strength — aluminum | 8 | N/mm² | ISO 4587; equivalent source value 1,200 psi |
| Impact strength | 3–7 | kJ/m² | ASTM D950 |
| Hardness | 85 | Shore D | ISO 868 |
| Dielectric strength | 250 | V/mil | Typical cured electrical property |
| Minimum exposure temperature | -55 | °C | Depends on the bonded materials; equivalent source value -65 °F |