PERMABOND 2050
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Toughened Structural Bonding
- 1,200 to 1,800 mPa s Viscosity Range
- 5 to 15-Second Fixturing Time
Product Description
PERMABOND® 2050 Flexible Cyanoacrylate Adhesive is a medium-high-viscosity, single-component ethyl cyanoacrylate adhesive designed for flexible, semi-porous, and dissimilar-material bonding. Its toughened formulation provides improved peel performance together with resistance to impact, vibration, thermal shock, and thermal cycling. The adhesive has a viscosity of 1,200–1,800 mPa·s at 25 °C and fills gaps up to 0.2 mm. Typical handling strength is reached in 5–15 seconds depending on the substrate, with full strength developing in 24 hours. It is suitable for plastics, elastomers, and metal assemblies where a more flexible instant adhesive bond is required.
Key features
- Flexible, toughened formulation: Provides improved peel strength and resistance to impact, vibration, thermal shock, and thermal cycling.
- Fast fixture performance: Typical handling strength is reached in 5–15 seconds depending on the bonded substrate.
- Controlled medium-high viscosity: A viscosity of 1,200–1,800 mPa·s supports accurate dispensing and gap filling up to 0.2 mm.
Applications / Suitable for
- Bonding flexible or semi-porous surfaces
- Bonding dissimilar materials
- Assemblies exposed to vibration or impact
- Applications exposed to thermal shock or thermal cycling
- Bonding plastics, elastomers, and metals
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical uncured and curing properties. Values are guideline information and do not constitute product specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical composition | Ethyl cyanoacrylate | — | Single-component adhesive |
| Appearance | Colorless liquid | — | As supplied |
| Viscosity | 1,200–1,800 | mPa·s | At 25 °C; equivalent to cP |
| Specific gravity | 1.1 | — | Typical uncured value |
| Maximum gap fill | 0.2 | mm | Equivalent source value 0.008 in |
| Fixture time — steel | 10–15 | s | Time to 0.3 N/mm² shear strength |
| Fixture time — Buna N rubber | 5–10 | s | Time to 0.3 N/mm² shear strength |
| Fixture time — PVC | 5–10 | s | Time to 0.3 N/mm² shear strength |
| Full strength | 24 | h | Typical full-strength development |
As-supplied / before-processing properties
Typical uncured and curing properties. Values are guideline information and do not constitute product specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical composition | Ethyl cyanoacrylate | — | Single-component adhesive |
| Appearance | Colorless liquid | — | As supplied |
| Viscosity | 1,200–1,800 | mPa·s | At 25 °C; equivalent to cP |
| Specific gravity | 1.1 | — | Typical uncured value |
| Maximum gap fill | 0.2 | mm | Equivalent source value 0.008 in |
| Fixture time — steel | 10–15 | s | Time to 0.3 N/mm² shear strength |
| Fixture time — Buna N rubber | 5–10 | s | Time to 0.3 N/mm² shear strength |
| Fixture time — PVC | 5–10 | s | Time to 0.3 N/mm² shear strength |
| Full strength | 24 | h | Typical full-strength development |