PERMABOND 41
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- 30-Minute On-Part Life
- Brush, Wipe, or Spray
- No-Mix Acrylic Initiation
Product Description
PERMABOND Initiator 41 functions as an amber, solvent-free surface initiator for compatible PERMABOND TA structural acrylic adhesives in no-mix bonding systems. The liquid is applied in a thin film by brush, wipe, or spray to one mating surface, while the adhesive is applied to the other. Assembly begins when the parts are brought together, eliminating a separate resin-and-initiator mixing step. The treated surface remains active for up to 30 minutes. With a typical specific gravity of 1.0 and 90 deg C flash point, Initiator 41 requires a compatible TA adhesive to form the bond.
Key features
- No-mix acrylic initiation: Activates compatible PERMABOND TA structural acrylic adhesives when coated parts are assembled.
- Thirty-minute on-part life: The treated surface remains active for up to 30 minutes before mating.
- Flexible application method: Supports brush, wipe, or spray application as a thin surface film.
Applications / Suitable for
- Initiating compatible PERMABOND TA structural acrylic adhesives
- No-mix bonding with initiator on one surface and adhesive on the other
- Brush, wipe, or spray surface application
TDS, SDS & Technical Documents
Technical Specifications
Other Properties
General Properties
Physical Properties
Thermal Properties
Additional Information
As-supplied and working properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Amber liquid | As supplied | |
| Specific gravity | 1.0 | Typical | |
| Flash point | 90 | deg C | Typical |
| On-part life | 30 | min | Treated surface |