PERMABOND 738
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Toughened cyanoacrylate formulation
- Approximately 5,000 mPa·s viscosity
- Suited to dark assemblies
Product Description
PERMABOND® 738 Toughened Cyanoacrylate Adhesive is a black, high-viscosity, single-component cyanoacrylate adhesive formulated to provide improved impact and peel performance compared with conventional cyanoacrylates. Its approximately 5,000 mPa·s viscosity supports controlled dispensing and gap filling up to 0.51 mm, while the black formulation is suited to dark-colored assemblies where adhesive appearance is important. PERMABOND® 738 adheres to substrates including steel, aluminum, galvanized steel, selected plastics, and elastomers. The TDS identifies speaker assembly, bonding to black substrates, and black PVC wire bonding as typical applications.
Key features
- Toughened performance: Formulated for improved impact and peel strength compared with conventional cyanoacrylate adhesives.
- High-viscosity gap filling: Approximately 5,000 mPa·s viscosity supports controlled application and gaps up to 0.51 mm.
- Black formulation: Designed to visually match dark substrates in applications such as speaker assemblies and black PVC wire bonding.
Applications / Suitable for
- Speaker assembly
- Bonding to black or dark-colored substrates
- Black PVC wire bonding
- Steel, aluminum, and galvanized-steel bonding
- Selected plastic and elastomer bonding
- Assemblies requiring improved impact or peel performance
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Curing Conditions
Mechanical Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical uncured and curing properties reported in the supplied technical datasheet. Values are representative and should not be treated as product specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Black liquid | — | As supplied |
| Solids content | 100 | % | TDS typical value |
| Viscosity | 5,000 | mPa·s | At 25 °C; source value 5,000 cP |
| Specific gravity | 1.1 | — | Typical uncured value |
| Flash point | 83 | °C | Equivalent source value 181 °F |
| Maximum gap fill | 0.51 | mm | Equivalent source value 0.020 in |
| Set time — steel | 25–30 | s | 25 °C; substrate-dependent cure-rate table |
| Set time — aluminum | 30–35 | s | 25 °C; substrate-dependent cure-rate table |
| Set time — phenolic | 5–10 | s | 25 °C; substrate-dependent cure-rate table |
| Set time — Buna rubber | 10–15 | s | 25 °C; substrate-dependent cure-rate table |
| Full cure | 24 | h | Typical full-cure time |
| Shelf life | 6 | months | Stored at 2–7 °C |
After-processing / final-state properties
Typical cured and bonded performance values from the supplied TDS. Bond strength varies with substrate, surface preparation, bond gap, humidity, and cure conditions.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Lap shear strength — grit-blasted steel | 21.4 | MPa | 24 h at room temperature; equivalent source value 3,100 psi |
| Lap shear — rigid PVC/PVC | Substrate failure | — | 24 h at room temperature |
| Lap shear — acrylic/acrylic | Substrate failure | — | 24 h at room temperature |
| Lap shear — polycarbonate/polycarbonate | Substrate failure | — | 24 h at room temperature |
| 180° peel strength — steel | 13.0 | pli | ASTM D903; sandblasted steel |
| Impact resistance — steel/steel | 8.0 | ft·lb/in² | ASTM D950 |
| PVC plasticizer resistance — flexible PVC/steel | Substrate failure | — | ASTM D903; 1 week at 70 °C |
| PVC plasticizer resistance — flexible PVC/PVC | Substrate failure | — | ASTM D1876 T-peel; 1 week at 70 °C |
| Hardness | 85 | Shore A | As reported in supplied TDS |
| Dielectric strength | 250 | V/mil | Approximate cured value |
| Operating temperature | -60 to 82 | °C | Performance/physical-property tables; see review flag regarding conflicting thermal statement |