PERMABOND 790
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- 2 to 3-Second Handling Time
- Surface-Insensitive Acidic-Substrate Bonding
- Low-Viscosity Wicking Post-Assembly Bonding
Product Description
Permabond® 790 Cyanoacrylate is an extremely fast-setting, low-viscosity, surface-insensitive adhesive designed to rapidly bond a wide variety of substrates. Its specialized formulation readily bonds acidic surfaces such as wood and plated metals, along with plastics, ceramics, and elastomers. Featuring a highly penetrative wicking viscosity, this 100% reactive, solvent-free adhesive is ideal for post-assembly applications and minimizes the occurrence of frosting and fogging during cure.
Key features
- Extremely fast setting: Single-component formula polymerizes rapidly upon contact with surface moisture, delivering fixture handling times of 2-3 seconds on steel and rubber.
- Surface insensitive: Expertly engineered to rapidly bond notoriously difficult acidic surfaces, including wood and plated materials.
- Low wicking viscosity: The exceptionally low 2 cP viscosity enables superior wicking action, making it perfectly suited for post-assembly penetration and application.
Applications / Suitable for
- Bonding acidic surfaces such as wood and plated materials
- Adhering plastics, metals, ceramics, and elastomers
- Post-assembly applications utilizing wicking penetration
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical Composition | Ethyl cyanoacrylate | - | - |
| Appearance | Colorless | - | - |
| Viscosity | 2 | cP | at 25°C (mPa.s) |
| Specific Gravity | 1.1 | - | - |
| Maximum Gap Fill | 0.05 | mm | (0.002 in) |
After-processing / final-state properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Fixture/Handling Time | 2-3 | seconds | Steel, Buna N Rubber, Phenolic |
| Full Strength | 24 | hours | - |
| Shear Strength | 18-22 | N/mm² | Steel (ISO 4587) (2600-3200 psi) |
| Impact Strength | 3-5 | kJ/m² | ASTM D-950 (1.4-2.4 ft-lb/in²) |
| Hardness | 85 | Shore D | ISO 868 |
| Dielectric Constant | 2.5 | - | at 10kHz |
| Dielectric Strength | 25 | kV/mm | - |