PERMABOND 922
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Up to 250 deg C Service
- Up to 0.4 mm Gap Filling
- MIL-A-46050C Type V Class 3 Approval
Product Description
Permabond® 922 Cyanoacrylate is an allyl-based, moderate-viscosity adhesive designed to provide both rapid bonding and extreme high-temperature resistance. This single-part, solvent-free liquid cures in seconds at room temperature but incorporates a secondary heat-activated curing mechanism. Following a specific post-cure schedule at 150°C (302°F), the adhesive forms highly durable bonds capable of withstanding environmental temperatures up to 250°C (482°F).
Key features
- Extreme temperature resistance: Secondary thermal curing enables the bonded assembly to continuously withstand temperatures up to 250°C (482°F).
- Moderate viscosity: The 1,200-2,000 cP viscosity is formulated to bridge larger gaps up to 0.4 mm while maintaining fast fixture times.
- Industry approved: Certified to MIL-A-46050C Type V Class 3 specifications for existing designs, ensuring reliable performance in demanding applications.
Applications / Suitable for
- High-temperature environments requiring continuous resistance up to 250°C after post-cure
- Bonding metals (steel, aluminum), plastics, and rubbers
- Applications requiring moderate gap filling capabilities up to 0.4 mm
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical Composition | Allyl cyanoacrylate | - | - |
| Appearance | Colorless | - | Liquid |
| Viscosity | 1,200-2,000 | cP | at 25°C (mPa.s) |
| Specific Gravity | 1.1 | - | - |
| Maximum Gap Fill | 0.4 | mm | (0.017 in) |
| Flash Point | 95 | °C | - |
| Volatile Organic Compound | < 2 | % | 20 g/L (Estimated) |
After-processing / final-state properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Fixture/Handling Time | < 20 | seconds | Steel |
| Full Strength | 24 | hours | - |
| Shear Strength | 19-23 | N/mm² | Steel (ISO 4587) (2800-3300 psi) |
| Impact Strength | 3-5 | kJ/m² | ASTM D-950 (1.4-2.4 ft-lb/in²) |
| Hardness | 85 | Shore D | ISO 868 |
| Coefficient of Thermal Expansion | 90E-6 | mm/mm/°C | - |
| Coefficient of Thermal Conductivity | 0.1 | W/(m.K) | - |
| Post-Cured Temperature Resistance | 250 | °C | (482°F) after thermal activation |