PERMABOND ET5145

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

PERMABOND ET5145

Main features

  • FDA 175.105/175.300 Compliance
  • Impact-Resistant Structural Bonding
  • 50 to 80-Minute Pot Life

Product Description

Permabond® ET5145 is a 1:1 mixable, two-part epoxy adhesive formulated with excellent environmental durability and resistance to impact and vibration. Specifically designed for high-strength structural bonding of metals, woods, composites, and certain plastics, this epoxy uniquely meets the strict requirements of FDA 175.105 and 175.300. This makes it highly suitable for manufacturing and assembly applications where the cured adhesive may come into contact with food or beverages.

Key features

  • FDA Compliant: Formulated to meet FDA 175.105 and 175.300 standards for safe use in food and beverage contact applications.
  • High structural strength: Provides excellent shear and peel strength across a wide variety of substrates, alongside robust impact and vibration resistance.
  • Room temperature cure: Offers a convenient 1:1 mix ratio and cures fully at room temperature, while boasting a long 50-80 minute pot life for complex assemblies.

Applications / Suitable for

  • Applications requiring FDA compliance for food or beverage contact
  • Structural bonding of metal, wood, composites, and certain plastics
  • Assemblies subjected to high impact, vibration, and harsh environmental conditions
Product Family

PERMABOND ET5145

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type Chemistry Type
A:Epoxy Resin/B:Polyamine Hardener
Mix Ratio Mix Ratio
1:1
Solids Solids
100 %
Specific Gravity Specific Gravity
A:1.3/ B:1.3
Work life @25°C Work life @25°C
50 - 80 min hours
Physical Properties
Viscosity (Part A) Viscosity (Part A)
50,000- 80,000 mPa.s mPa.s
Viscosity (Part B) Viscosity (Part B)
100,000- 200,000 mPa.s
Mechanical Properties
Peel Strength Peel Strength
30-50 N/25mm
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
40-50 °C
Electrical Properties
Dielectric Strength Dielectric Strength
15-25 kV/mm
Other Properties
Maximum gap fill Maximum gap fill
2 mm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Mix Ratio by Volume 1:1 - -
Chemical Composition Epoxy Resin - Part A (ET5145A)
Chemical Composition Polyamine Hardener - Part B (ET5145B)
Appearance White - Part A (ET5145A)
Appearance Ivory - Part B (ET5145B)
Viscosity (Part A) 50,000-80,000 cP at 25°C, 20rpm
Viscosity (Part A) 200,000-300,000 cP at 25°C, 2rpm
Viscosity (Part B) 100,000-200,000 cP at 25°C, 20rpm
Viscosity (Part B) 250,000-400,000 cP at 25°C, 2rpm
Specific Gravity 1.3 - Part A and Part B
Maximum Gap Fill 2 mm (0.08 in)
Usable / Pot Life 50-80 minutes at 23°C (1+1g)
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Handling Time 3-5 hours at 23°C
Working Strength 16 hours at 23°C
Working Strength 30 minutes at 60°C
Full Cure 72 hours at 23°C
Full Cure 1 hour at 60°C
Shear Strength 19-21 N/mm² Mild steel (ISO 4587) (2800-3000 psi)
Shear Strength 18-21 N/mm² Stainless steel (ISO 4587) (2600-3000 psi)
Shear Strength 10-14 N/mm² Aluminium (ISO 4587) (1450-2000 psi)
Peel Strength 30-50 N/25mm Aluminium (ISO 4578) (7-11 PIW)
Hardness 75-85 Shore D ISO 868
Glass Transition Temperature (Tg) 40-50 °C (104-122°F)
Dielectric Strength 15-25 kV/mm -