PERMABOND QFS16
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- 5-Second Steel Set Time
- Faster Cure Through Gaps
- Reduced Plastic Stress Cracking
Product Description
Permabond QFS16 is a colorless cyanoacrylate activator for shortening set time on closely mated parts, porous surfaces, gaps, and wire-tacking assemblies. It is applied to one component by wiping, spraying, or dipping and allowed to evaporate before adhesive is placed on the untreated surface. With a 100 cP ethyl-2-cyanoacrylate at 23 deg C, typical set time is 5 seconds on gap-free steel and 40-60 seconds across a 5 mil gap. The formulation also reduces stress cracking, surface discoloration, and adhesive frosting on supported plastic parts.
Key features
- Rapid Steel Set: Provides a typical 5-second set on gap-free steel under stated conditions.
- Gap and Porous-Surface Cure: Accelerates cyanoacrylate cure through gaps and on porous materials.
- Reduced Plastic Surface Effects: Helps limit stress cracking, discoloration, and frosting on supported plastics.
Applications
Applications include porous or poorly mated parts, gap bonding, wire tacking, excess-fillet cure, and supported plastic assemblies.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Other Properties
Additional Information
As supplied / before processing
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product type | Cyanoacrylate activator | As supplied | |
| Color | Colorless | As supplied | |
| Specific gravity | 0.68 | As supplied | |
| Flash point | -2 | deg C | As supplied |
| Application method | Wipe, spray, or dip one component | Allow full evaporation before bonding | |
| Storage temperature | 5 to 25 | deg C | Recommended storage range |
After processing / final state
Set-time values apply to 100 cP ethyl-2-cyanoacrylate at 23 deg C; the control row is identified separately.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Set time - steel, no gap | 5 | seconds | At 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16 |
| Set time - steel, 5 mil gap | 40-60 | seconds | At 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16 |
| Set time - steel, no gap, control | 10-15 | seconds | At 23 deg C without QFS16 |
| Set time - Buna-N, no gap | 10 | seconds | At 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16 |
| Set time - phenolic, no gap | 5 | seconds | At 23 deg C with 100 cP ethyl-2-cyanoacrylate and QFS16 |