PERMABOND TA4810
Harmonization Code : 3904.61.00.00 | Polytetrafluoroethylene plates / sheets / film / tape / strip, self-adhesive, in rolls
Main features
- As-Received Metal Bonding
- Non-Sag 2 mm Gap Filling
- Fast Working-Strength Development
Product Description
Permabond TA4810 is a two-part, 1:1 toughened methacrylate adhesive for structural bonding of thermoplastics, thermosets, metals, and composites. It is formulated for adhesion to as-received metal surfaces and combines thixotropic static-mixer dispensing with non-sag gap filling up to 2 mm. At 23 deg C, typical pot life is 4 to 6 minutes, fixture time is 10 to 15 minutes, and working strength develops in 50 to 60 minutes. It also provides resistance to many common industrial solvents and fuels and is intended for harsh environmental conditions.
Key features
- As-Received Metal Adhesion: Supports high-strength bonding to as-received metal surfaces.
- Non-Sag 2 mm Gap Fill: Thixotropic flow supports static-mixer dispensing and gap filling without sag.
- Fast Working-Strength Build: Develops typical working strength in 50 to 60 minutes at 23 deg C.
Applications
Applications include structural bonding of thermoplastics, thermosets, metals, composites, and mixed-material assemblies.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Curing Conditions
Mechanical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Values identify the separate Part A and Part B components or the mixed adhesive, as stated.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Part A viscosity | 150,000 to 230,000 | mPa s | At 25 deg C |
| Part B viscosity | 120,000 to 200,000 | mPa s | At 25 deg C |
| Mix ratio | 1:1 | Part A to Part B | |
| Maximum gap fill | 2 | mm | Typical curing property |
| Pot life | 4 to 6 | minutes | 10 g + 10 g at 23 deg C |
| Fixture time | 10 to 15 | minutes | At 23 deg C |
| Handling time | 20 to 30 | minutes | 0.3 N/mm^2 shear strength at 23 deg C |
| Working strength | 50 to 60 | minutes | At 23 deg C |
After-processing / final-state properties
Strength and electrical values are typical cured results for the stated methods and substrates.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shear strength - steel | 21 to 28 | N/mm^2 | ISO 4587 |
| Shear strength - aluminum | 14 to 22 | N/mm^2 | ISO 4587 |
| Shear strength - fiberglass | >12 | N/mm^2 | ISO 4587 |
| Tensile strength | 29 | N/mm^2 | ISO 37 |
| Peel strength | 70 to 90 | N/25 mm | ISO 4578 |
| Elongation | 15 to 20 | % | ISO 37 |
| Dielectric strength | 30 to 50 | kV/mm | ASTM D-149 |
| Volume resistivity | 2 x 10^13 | ohm cm | ASTM D-257 |