PERMABOND TA4811
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- 1:1 toughened methacrylate chemistry
- Fast room-temperature cure
- Durable structural performance
Product Description
PERMABOND TA4811 is a two-part, 1:1 toughened methacrylate structural adhesive designed for bonding thermoplastics, thermosets, metals, and composites. The adhesive develops strong bonds to a wide range of substrates, including as-received metal surfaces without surface preparation. TA4811 cures rapidly at room temperature and features thixotropic, non-sag characteristics that support easy dispensing through static mixers while maintaining gap-filling capability. The cured adhesive offers high shear and peel strength, good impact resistance, chemical resistance, and durability in demanding industrial environments.
Key features
- 1:1 toughened methacrylate chemistry: Simplifies mixing and dispensing while supporting reliable structural bonding.
- Fast room-temperature cure: Provides a 4-6 minute working time, 10-15 minute fixture time, and full cure within 24 hours.
- Durable structural performance: Delivers high shear strength along with good impact, chemical, and environmental resistance.
Applications / Suitable for
- Bonding thermoplastics
- Bonding thermoset materials
- Metal assembly applications
- Composite component bonding
- Industrial assemblies requiring gap-filling and non-sag adhesive performance
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Curing Conditions
Mechanical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical uncured adhesive and processing properties.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Mix ratio | 1:1 | - | Part A : Part B |
| Mixed viscosity | 90,000-100,000 | cP | @ 25°C |
| Working time | 4-6 | minutes | Typical |
| Fixture time | 10-15 | minutes | Typical |
| Maximum gap fill | 2 | mm | Typical |
| Full cure | 24 | hours | Room temperature |
After-processing / final-state properties
Typical cured adhesive performance properties.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shear strength (steel) | 3,500-4,500 | psi | ASTM D1002 |
| Shear strength (aluminum) | 3,000-4,000 | psi | ASTM D1002 |
| Tensile strength | 4,200 | psi | DIN 53283 |
| Peel strength | 15-20 | pli | Typical |
| Elongation | 15-20 | % | Typical |
| Thermal conductivity | 0.1 | W/m·K | ASTM C177 |