PLEXUS H4110
Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics
Main features
- Extended 8-12 Minute Work Window
- Non-Sag Gel Placement
- Elastic Mixed-Material Bonding
Product Description
Plexus H4110 is a two-part, 1:1 hybrid adhesive supplied as a non-sagging gel for elastic semi-structural bonding. It provides an 8-12 minute work time at 25 deg C for positioning composites, thermoplastics, metals, wood, concrete, and cement. The low-odor, low-exotherm formulation supports controlled application where a more elastic bond is preferred over a rigid structural joint. Its gel consistency limits slump during placement and keeps the mixed adhesive within the intended bond area across supported mixed-material assemblies.
Key features
- 8-12 Minute Work Window: Allows measured part positioning at 25 deg C.
- Non-Sag Gel Control: Maintains controlled placement during assembly.
- Elastic Semi-Structural Bond: Forms an elastic bond for supported mixed-material assemblies.
Applications
Applications include bonding composites, thermoplastics, metals, wood, concrete, and cement.
TDS, SDS & Technical Documents
Technical Specifications
Physical Properties
Mechanical Properties
General Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| System form | Two-part non-sagging gel | As supplied and mixed for application | |
| Mix ratio by volume | 1:1 | Adhesive to activator | |
| Work time | 8-12 | minutes | At 25 deg C |
| Exotherm characteristic | Low | Mixed adhesive | |
| Odor characteristic | Low | Mixed adhesive |