Hardman Double/Bubble 04007 Very High Peel Strength Epoxy is a 3.5 g premeasured, two-part structural epoxy packet with a semi-rigid cured profile and high peel performance. The gray mixed adhesive has a 50,000 cP viscosity at 25 deg C, a 3 hour work time, and an 18 hour handling time. After a 7 day cure at 25 deg C, typical T-peel strength reaches 24 pli and lap shear strength reaches 2,800 psi on acid-etched aluminum. The cured material has 65 Shore D hardness and a maximum service temperature of 121 deg C. It is used for repair and bonding where vibration, impact, shock, or peel loading is important.

Key features

  • High-peel semi-rigid cure: Typical T-peel strength is 24 pli on acid-etched aluminum after a 7 day cure at 25 deg C.
  • Extended 3-hour work time: The long open window supports placement and alignment before handling.
  • Elevated-temperature capability: The cured adhesive has a maximum service temperature of 121 deg C.

Applications

Applications include structural bonding and repair of industrial parts, sports equipment, marine and transportation parts, grinding-wheel hubs, and door or window gaskets where peel, vibration, impact, or shock resistance is required.

Product Family

ROYAL DOUBLE BUBBLE 04007

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Service temperature Service temperature
121 °C

Additional Information

Technical properties

As supplied / before processing

Property Value Unit Method / condition
Package size3.5gPremeasured dual-pouch packet
ColorGray-Mixed adhesive
Mixed viscosity50,000cPAt 25 deg C
Mixed specific gravity1.27-At 25 deg C
Work time3hAt room temperature
Handling strength18hAt room temperature
Shelf life24monthsPart A and Part B
Technical properties

After processing / final state

Property Value Unit Method / condition
Hardness65Shore DTested at 25 deg C
Maximum service temperature121deg CCured adhesive
Lap shear strength2,800psiAcid-etched aluminum-to-aluminum; 7 day cure at 25 deg C; tested at 25 deg C
T-peel strength24pliAcid-etched aluminum-to-aluminum; 7 day cure at 25 deg C; tested at 25 deg C
Lap shear strength3,206psiAcid-etched aluminum-to-aluminum; 7 day cure at 25 deg C; tested at -40 deg C
Lap shear strength970psiAcid-etched aluminum-to-aluminum; 7 day cure at 25 deg C; tested at 82 deg C