ROYAL RP-5
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Fast-setting general-purpose adhesive with 5-second fixture
- Low 5 cps viscosity
- Grit-blasted steel shear strength of 28 N/mm²
Product Description
RP5 General Purpose Adhesive is a medium-setting adhesive designed to bond a wide variety of similar and dissimilar materials. The clear, low-viscosity material has a reported viscosity of 5 cps and develops handling strength in 5 to 10 seconds, with full cure in 8 hours. The product is described as providing climatic, thermal, and impact resistance, while its elasticity supports bonding between dissimilar materials. Documented strength testing includes steel, aluminum, ABS, PVC, polycarbonate, phenolic, neoprene rubber, and nitrile rubber substrates.
Key features
- Fast fixture and handling: Fixture cure is reported at 5 seconds, with handling strength developing in approximately 5 to 10 seconds.
- Low-viscosity formulation: 5 cps viscosity supports application where a low-viscosity adhesive is required.
- Broad documented substrate testing: Strength data are provided for metals, engineering plastics, phenolic, and rubber substrates.
Applications / Suitable for
- General-purpose bonding of similar or dissimilar materials
- Bonding applications involving metals, plastics, phenolic, and rubber substrates represented in the documented test data
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Selected physical and processing properties of RP5 before full cure.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Clear | - | As supplied |
| Base | Ethyl | - | Source terminology |
| Viscosity | 5 | cps | Physical property |
| Specific gravity | 1.05 | - | Physical property |
| Fixture cure | 5 | seconds | Reported cure speed for fixture |
| Handling strength | 5 to 10 | seconds | Reported handling-strength development |
| Full cure | 8 | hours | Reported full-cure time |
After-processing / final-state properties
Selected cured adhesive strength and temperature data for RP5 under the stated substrate and test configurations.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shear strength | 28; range 24 to 32 | N/mm² | Grit-blasted steel; ASTM D1002 / DIN 53283 |
| Shear strength | 20; range 16 to 24 | N/mm² | Etched aluminum; ASTM D1002 / DIN 53283 |
| Shear strength | >7 / >5 / >6 | N/mm² | ABS / PVC / polycarbonate; ASTM D1002 / DIN 53283; substrate failure noted |
| Shear strength | >12 | N/mm² | Neoprene rubber and nitrile rubber; ASTM D1002 / DIN 53283; substrate failure noted |
| Tensile strength | 20; range 14 to 28 | N/mm² | Grit-blasted steel; ASTM D2095 / DIN 53283 |
| Temperature range | -65 to 200 | °F | Reported physical property |