SIKA SIKALASTOMER- 511 NON-SKINNING BUTYL SEALANT
Harmonization Code : 8547.90.00.00 | Insulating fittings for electrical machines, appliances or equipment, being fittings wholly of insulating material apart from any minor components of metal (for example, threaded sockets) incorporated during moulding solely for purposes of assembly, other than insulators of heading 8546; electrical conduit tubing and joints therefor, of base metal
Main features
- Non-Corrosive Sealing Formulation
- Standing-Seam Roof and Wall-Panel Sealing
- 50 to 105 deg C Service Range
Product Description
SikaLastomer®-511 is a one-part, non-skinning and non-corrosive butyl-rubber sealant for factory sealing standing-seam roof and wall panels and concealed end laps. The off-white material remains malleable after application, allowing metal panels to be separated later for repair or maintenance. It is applied to clean surfaces using manual, pneumatic, electric, or pump equipment within a documented application-temperature range of 5°C to 40°C. The sealant has a typical uncured density of 1.09 kg/L and a service-temperature range of -50°C to 105°C.
Key features
- Non-skinning butyl sealant: The material remains malleable after application and supports later panel separation.
- Factory-to-field assembly window: Panels may be joined in the field up to six months after initial application under the documented conditions.
- Wide service range: The documented service-temperature range is -50°C to 105°C.
Applications / Suitable for
- Factory sealing of standing-seam roof panels
- Standing-seam wall panels
- Concealed panel end laps
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Chemical base | Butyl | N/A | As supplied |
| Color | Off-white | N/A | CQP001-1 |
| Uncured density | 1.09 | kg/L | Typical product data |
| Application temperature | 5 to 40 | °C | Ambient |
| Slump | 1 | mm | ASTM D2202 at 23°C and 50% RH |
| Shelf life | 12 | months | Cartridges, pails, or drums stored below 25°C |
After-processing / final-state properties
Typical final-state values under the stated system and test conditions. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Service temperature | -50 to 105 | °C | Documented range |
| Shrinkage | 16 | % | CQP014-1 |
| Heat-aging weight loss | 11 | % | ASTM C792 |
| Staining | No staining | N/A | ASTM D925 on common substrates |