HLT 7000 | Two part Hybrid Thermal Gel

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

HLT 7000 | Two part Hybrid Thermal Gel HLT 7000 | Two part Hybrid Thermal Gel

Main features

  • Dark Red + Gray
  • 7.0 Thermal Conductivity
  • High reliability

Product Description

Honeywell HLT 7000 High TC Hybrid TIM is a two-component, dispensable thermal gap filler, which offers high thermal conductivity and long-term reliability. This product is easy to dispense and rework, making it ideal for high volume manufacturing.

Honeywell HLT 7000 marks the start of the High end TIM product line. It has a thermal conductivity of 7.0 W/mK accompanied with high reliability and ease of dispense. It can be cured after two-component mixing and can be cured faster under higher temperature. Its high compressibility minimizes thermal resistance at interfaces, while maintaining excellent performance during reliability testing.

You probably noticed the lack of information and product properties. Since those are top notch products, we go to certain extends to protect Honeywell's IP and competitive advantages. A plethora of information,  including additional data,  images and samples are available once an NDA is in place. Contact us for more details.

Product Family

SOLSTICE HLT7000

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
Dark Red - Gray
Thermal Properties
Thermal Conductivity Thermal Conductivity
7.0 W/m.K

Leading Brands Trust in Our Products and Services