PTM 5000-SP | Phase Change Paste
Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other
Main features
- 0.06 - 0.08 Thermal Impedance
- 3.5 - 4.5 Thermal Conductivity
- Stencil Printable
Product Description
PTM5000-SP is Honeywell's thermally conductive phase change paste, which is available in Stencil printable form. It is designed to minimize thermal resistance at interfaces and maintain extremely stable performance through reliability testing required for long product life applications.
PTM5000-SP has a Thermal conductivity of 3.5 - 4.5 (W/m·K) depending on the bondline thickness and is based on a robust polymer PCM structure that exhibits excellent wetting properties during typical operating temperature ranges, resulting in very low surface contact resistance. The proprietary material provides superior reliability and maintains low thermal impedance (0.06-0.08) , making it desirable for high-performance integrated circuit devices.
Packaging
TDS, SDS & Technical Documents
- Honeywell PTM 5000-SP SDS
- IGBT Printing process guideline
- PTM5000_TDS_2023
- Honeywell_1907_2006 _SVHC Compliance_2024
- HEMTIMApplicationNoteSPtype
- PTM5000-SP_HL_202503_REPORT_NO_6169633
- PTM5000-SP_HL_202503_REPORT_NO_6169628
- PTM5000-SP_HL_202503_REPORT_NO_6169631
- PTM5000-SP_HL_202503_REPORT_NO_6169630
- CAPLINQ Honeywell Phase Change Material Troubleshooting Guide v2
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Additional Information
ROHS Compliance
The following SGS Test Reports strongly supports that PTM5000 material remains within ROHS limits:
PTM5000-SP_HL_202503_REPORT_NO_6169628
PTM5000-SP_HL_202503_REPORT_NO_6169630
PTM5000-SP_HL_202503_REPORT_NO_6169631
PTM5000-SP_HL_202503_REPORT_NO_6169633
When choosing a printable paste it is important to understand the process parameters and limitations.
That's why we ask, when you contact us, to include the following information:
- What is your print thickness?
- How long is your printing time and working window?
- What is your drying step after printing?
- Temperature (Room temperature or something else?)
- Time
- Do you have any viscosity limitations in the printing process?