TGP1500 | Thermal Gap Pad

Main features

  • 0.94 Thermal Impedance
  • 1.5 Thermal Conductivity
  • 0.5 - 5 mm Thickness

Product Description

Honeywell's TGP1500 Thermal Gap Pads (TGP) are low cost materials, comparable to TGP1200 with better thermal performance and ease of use across a multitude of applications. Their ultra-high compressibility enables low stress and excellent conformity to mating surfaces. They are designed to minimize thermal resistance at interfaces, and maintain excellent performance through reliability testing. They have a very competitive cost of ownership and are ideal for not extremely demanding applications.

Honeywell's TGP1500 is naturally tacky, and requires no additional adhesive which could inhibit thermal performance. Products have very low hardness and are available in a thickness range from 0.5mm to 5.0mm.

 

Product Family

SOLSTICE TGP1500

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 16 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
Grey
Film Thickness Film Thickness
0.5 - 5 mm
Specific Gravity Specific Gravity
1.8
Thermal Properties
Thermal Conductivity Thermal Conductivity
1.5 W/m.K
Thermal Impedance Thermal Impedance
0.94 °C·cm²/W
UL 94 Rating UL 94 Rating
V-0
Electrical Properties
Volume Resistivity Volume Resistivity
20000000000000 Ohms⋅cm

Additional Information

 

alt

 

Thickness range:

  • 0.5-5.0mm with 0.25mm incremental

 

Thickness Tolerance: >1mm, ±10%

  • 0.5-1mm, ±0.1mm
  • <0.5mm, ±0.05mm