Loctite STYCAST 2651-40W1
Harmonization Code : 3907.30.00.15 | Epoxide resin, halogen-free
Main features
- Epoxy Potting and Encapsulation Resin
- Room-Temperature Encapsulation Cure
- 0.5 W/(m K) Thermal Encapsulation
Product Description
LOCTITE® STYCAST 2651-40 W1 GOLD is a gold-colored epoxy resin for general potting and encapsulation of metal, plastic, and ceramic assemblies. The material has a typical viscosity of 33,000 mPa·s at 25°C and may be combined with LOCTITE CAT 9 for room-temperature cure or LOCTITE CAT 11 for elevated-temperature cure. The selected catalyst changes mix ratio, pot life, coefficient of thermal expansion, moisture absorption, electrical properties, and operating-temperature range. After cure, the material is documented as machinable with carbide tools.
Key features
- General potting resin: The epoxy is documented for potting and encapsulation of metals, plastics, and ceramics.
- Two catalyst options: CAT 9 supports room-temperature cure, while CAT 11 supports elevated-temperature cure.
- Machinable cured material: The fully cured epoxy may be machined with carbide tools.
Applications / Suitable for
- General electrical and electronic potting
- Encapsulation of metal, plastic, and ceramic assemblies
- Castings requiring post-cure machining
TDS, SDS & Technical Documents
Technical Specifications
Physical Properties
General Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Gold | N/A | Resin as supplied |
| Viscosity | 33,000 | mPa·s | At 25°C |
| Density | 1.5 | g/cm³ | Resin as supplied |
| Shelf life | 365 | days | At 18°C to 25°C from date of manufacture |
| Mix ratio with CAT 9 | 100:8 to 9 | parts by weight | Resin : catalyst |
| Pot life with CAT 9 | 30 | min | Typical |
| Mix ratio with CAT 11 | 100:10 to 11 | parts by weight | Resin : catalyst |
| Pot life with CAT 11 | 4 | h | Typical |
After-processing / final-state properties
Typical final-state values under the stated system and test conditions. These values are not sales specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Hardness | 87.5 | Shore D | With CAT 9 |
| Thermal conductivity | 0.5 | W/m·K | With CAT 9 |
| CTE | 78 | ppm/°C | With CAT 9 |
| Operating temperature | -40 to 175 | °C | With CAT 9 |
| Hardness | 87.5 | Shore D | With CAT 11 |
| Thermal conductivity | 0.5 | W/m·K | With CAT 11 |
| CTE | 45 | ppm/°C | With CAT 11 |
| Operating temperature | -70 to 175 | °C | With CAT 11 |