Engineered Solutions for Modern Data Center Infrastructure

Reliable Performance for Next-Generation Compute Workloads

Direct-to-Chip Liquid Cooling for Data Centers

Jump to KRAYDEN Heat Transfer Liquid Solutions for Direct-to-Chip Cooling: Heat Transfer Fluids
 

The rapid growth of artificial intelligence (AI), Internet of Things (IoT), and high-performance computing workloads is driving a steady increase in power density in modern data centers. As server performance scales to support these workloads, power consumption rises and heat generation increases at both the rack level and, more critically, at the processor and accelerator level. Today, most data centers rely on air-based datacom equipment cooling systems (DECS) as the primary means of thermal management.

 
Data center air cooling using server fans, heat sinks, and hot-aisle cold-aisle airflow management

Typical air-cooled data center layout showing server racks, airflow paths, and hot-aisle/cold-aisle separation

Data Center Thermal Management via Air Cooling

Conventional Cooling Architecture for IT Infrastructure

Air cooling is the most widely deployed thermal management approach in data centers today. Heat generated by operating servers is conducted away from processors, memory, and power electronics through heat sinks. Airflow, driven by internal server fans, transports this heat out of the equipment.

The warmed exhaust air is routed back to facility-level cooling equipment such as computer room air conditioners (CRAC), which use refrigerant-based cooling, or computer room air handlers (CRAH), which rely on chilled water systems. The conditioned air is then recirculated to the IT equipment. To improve thermal efficiency and prevent air mixing, airflow paths are commonly organized using hot-aisle and cold-aisle containment strategies.

Cool Air Supply
→
Server Inlet
→
Heat Pickup
→
Warm Air Exhaust
→
CRAC / CRAH Cooling
→
Cool Air Recirculation

Closed-loop airflow cycle in air-cooled data center environments


These characteristics define how air cooling is deployed in data centers today, from its widespread adoption to its practical power-density limits.

~80% Market Share

Approximately 70–80% of data centers worldwide continue to rely on air cooling as their primary thermal management approach.

Low Power Density Applications

Air cooling is most commonly used in enterprise, colocation, edge, and legacy data center environments operating at lower rack power densities.

20–35 kW per Rack

Typical operation remains below ~20 kW per rack, with advanced airflow management and containment extending practical limits to ~30–35 kW.


Liquid Cooling Architectures in Modern Data Centers

Today’s high-performance server racks increasingly exceed 20, 30, and even 50 kW. As rack densities rise and heat becomes more concentrated at the processor and accelerator level, the limitations of air-based cooling become more pronounced. In response, data center operators are adopting liquid cooling to manage higher heat flux more efficiently. This shift complements, rather than replaces, air cooling and is commonly implemented through three primary architectures: direct-to-chip cooling, immersion cooling, and rear-door heat exchangers.

Direct-to-chip liquid cooling using cold plates mounted on CPUs and GPUs

Direct-to-Chip Liquid Cooling

Direct-to-chip cooling removes heat by circulating liquid coolant through cold plates mounted directly on CPUs, GPUs, and accelerators. Heat is extracted at the package level, minimizing thermal resistance and enabling efficient heat removal at the source.

Coolant absorbs heat inside the cold plate and circulates through a closed-loop system before transferring thermal energy to the facility cooling infrastructure.

Advantages

Lowest thermal resistance, efficient heat extraction at the processor level, and support for very high rack power densities.

Limitations

Requires liquid distribution infrastructure, coolant management, and careful material compatibility control.

Typical Applications

AI training clusters, HPC systems, and accelerator-dense racks where air cooling is no longer sufficient.

 
Immersion cooling with servers submerged in dielectric liquid

Immersion Cooling

Immersion cooling removes heat by submerging servers or components directly into a dielectric liquid. Heat transfers uniformly from exposed surfaces into the surrounding fluid.

This approach eliminates traditional heat sinks, fans, and internal airflow paths, enabling very high heat flux operation.

Advantages

Extremely high heat removal capability and simplified thermal paths.

Limitations

Requires purpose-built hardware, specialized fluids, and changes to service and maintenance workflows.

Typical Applications

Ultra-high-density deployments where maximum heat flux outweighs serviceability concerns.

 
Rear-door heat exchanger mounted on server racks

Rear-Door Heat Exchangers (RDHx)

Rear-door heat exchangers remove heat from server exhaust air using liquid-cooled coils mounted on the rear of racks.

Heat transfers from hot air to a liquid loop while servers remain air-cooled internally.

Advantages

Reduces room heat load and extends the usable range of air-cooled servers.

Limitations

Does not remove heat at the processor level; chip-level thermal bottlenecks remain.

Typical Applications

Retrofit and hybrid air–liquid environments seeking incremental thermal improvements.

 
Technology Insight

How Direct-to-Chip Cooling Works

 

In a direct-to-chip (D2C) cooling system, heat is removed through a closed-loop liquid path that begins at the processor and ends at the facility cooling system. By extracting heat directly at the chip level, this approach minimizes thermal resistance and enables significantly higher power densities compared to air-based cooling.

Heat transfer from processor into the cold plate

Step 1: Heat Capture at the Processor

Modern CPUs and GPUs generate high heat loads concentrated at the chip surface due to increasing power density.  Heat flows from the processor, through a thermal interface material, and into a liquid-cooled cold plate mounted directly on the CPU or GPU.

Coolant absorbing heat and exiting the cold plate

Step 2: Heat Absorption and Transport

Coolant flows through channels inside the cold plate and absorbs heat directly from the processor. Heat is absorbed by the coolant or heat transfer fluid.

In single-phase D2C cooling, the coolant remains in liquid form as it absorbs heat, and its temperature rises.

In two-phase D2C cooling, the coolant absorbs heat by partially changing phase (from liquid to vapor), allowing large amounts of heat to be removed at nearly constant temperature.

Heated coolant transported through the liquid cooling loop

Step 3: Heat Rejection to Facility Cooling

The warmed liquid (or liquid–vapor mixture in two-phase systems) leaves the cold plate and flows through the direct-to-chip cooling loop. Flow is controlled using pumps, manifolds, and valves. Heat carried by the coolant is transferred to the facility cooling system through a heat exchanger.

In single-phase systems, heat is rejected as the liquid is cooled back down. In two-phase systems, vapor condenses back into liquid during heat rejection before being recirculated.


Main Direct-to-Chip Liquid Cooling Components

 

Direct-to-chip cooling architecture showing cold plates, coolant flow, and heat removal at the processor level
Key Direct-to-Chip Liquid Cooling Components
1 Heat transfer fluid that absorbs heat at the cold plate and transports it through the liquid cooling loop.
2 Chip-level cooling hardware, including cold plates and thermal interface materials (TIMs), that transfer heat directly from CPUs and GPUs into the liquid.
3 Fluid distribution and flow-control components, such as manifolds, pumps, and tubing, that regulate coolant delivery through the liquid cooling loop.
4 Heat rejection interface, typically a liquid-to-liquid or liquid-to-air heat exchanger, that transfers heat from the rack-level liquid loop to the facility cooling system.
5 Monitoring and control systems, including temperature, pressure, and flow sensors, that ensure stable and reliable operation of the liquid cooling loop.

At the center of direct-to-chip liquid cooling is the heat transfer fluid, or coolant, which governs how effectively heat is managed once it leaves the processor. Beyond enabling heat removal at the cold plate, coolant properties determine thermal performance, materials compatibiity, and long-term reliability across the entire liquid cooling loop.


Key Heat Transfer Fluid Requirements for Direct-to-Chip Cooling

Thermal Performance

The primary function of a heat transfer fluid is to efficiently remove heat from high-power processors. Key thermal properties include high specific heat capacity to absorb large heat loads, sufficient thermal conductivity to minimize temperature gradients, and stable performance across the operating temperature range of the cooling loop.

These properties directly influence junction temperature, temperature uniformity across cold plates, and overall cooling efficiency at elevated rack power densities.

Fluid Flow and Pumping Behavior

Viscosity and flow behavior determine how easily the coolant can be circulated through cold plates, manifolds, and heat exchangers. Fluids with excessively high viscosity increase pumping power requirements and system energy consumption.

Optimized flow properties are essential for maintaining uniform coolant distribution, minimizing pressure drop, and enabling scalable cooling architectures as system complexity increases.

Materials Compatibility

Heat transfer fluids must be chemically compatible with a wide range of materials, including metals, elastomers, polymers, seals, and thermal interface materials used in direct-to-chip cooling systems.

Incompatible fluids can lead to corrosion, swelling, leaching, or degradation of system components, ultimately compromising reliability and increasing maintenance requirements.

Long-Term Stability and Reliability

Direct-to-chip cooling fluids must maintain stable physical and chemical properties over extended operating lifetimes. Resistance to oxidation, thermal degradation, and contamination is critical for long-term system performance.

Stable fluids reduce the risk of fouling, particulate formation, and performance drift, supporting predictable operation and minimizing downtime in mission-critical data center environments.

 

Enabling Reliable Thermal Management in High-Density Data Centers

Heat Transfer Fluids for Direct-to-Chip Cooling

DOWFROST™ LC 25

Ready-to-Use Propylene Glycol Heat Transfer Fluid (PG25, 25 vol%)

DOWFROST™ LC 25 is a ready-to-use 25 vol% propylene glycol (PG25) heat transfer fluid for HVAC, data-center cooling loops, process cooling, and direct-to-chip liquid cooling systems. The fluid contains a corrosion-inhibitor package designed to slow glycol oxidation, control pH, and protect common loop materials, including copper, brass, carbon steel, cast iron, and aluminum.

DOWFROST™ LC 25 is formulated using Dow PURAGUARD™ USP/EP-grade propylene glycol (>99.8% purity), reducing contaminants that contribute to odor, discoloration, and accelerated fluid degradation. High base-fluid purity improves chemical stability beyond what inhibitors alone can provide. The fluid is dyed fluorescent yellow-green for leak detection. Gradual color darkening may occur during service and is acceptable if the fluid remains clear and free of suspended solids.

Typical Properties

Propylene Glycol Concentration 25 vol%
Freezing Point 14 °F (–10 °C)
Boiling Point @ 760 mmHg 101.4 °C
Specific Gravity (25/25 °C) 1.030–1.036
pH 8.0–10.5
Reserve Alkalinity >6.0 mL 0.1 N HCl
Thermal Conductivity @ 50 °C 0.485 W/m·K
Specific Heat @ 50 °C 4.13 kJ/kg·K
Viscosity 2.72 mPa·s @ 20 °C
1.15 mPa·s @ 50 °C
Volume Expansion (–10 to 90 °C) 5.1 %
Sulfate Content <10 ppm
Chloride Content <5 ppm
Total Hardness (as CaCO₃) <20 ppm

Typical values shown for reference only and should not be used as specifications.

Applications

  • Datacom and telecom equipment cooling loops
  • Direct-to-chip liquid cooling for high-performance processors and accelerators
  • Data center thermal management and rack-level liquid cooling systems
  • HVAC and process cooling systems requiring long-term fluid stability
  • Suitable for systems where fluid cleanliness, material compatibility, and long-term corrosion control are critical
Direct-to-chip liquid cooling cold plate using DOWFROST LC25 heat transfer fluid

Corrosion Performance of DOWFROST™ LC 25

Long-term reliability of direct-to-chip liquid cooling systems depends on strict control of corrosion across all wetted materials. Comparative corrosion testing demonstrates that DOWFROST™ LC 25 delivers excellent corrosion protection across all metals tested, achieving orders-of-magnitude lower corrosion rates than water and uninhibited propylene glycol.

 

Corrosion comparison of water, uninhibited propylene glycol, and DOWFROST LC25 after ASTM D1384 testing

Visual comparison of metal corrosion after exposure to water, uninhibited propylene glycol, and DOWFROST LC 25

Key Findings

  • Extremely low corrosion rates across copper, steel, iron, brass, solder, and aluminum
  • Orders-of-magnitude improvement compared to water and uninhibited propylene glycol
  • All measured values fall well below commonly accepted corrosion thresholds
  • Suitable for mixed-metal liquid cooling loops in high-density data center environments
Metal Water (mpy) Uninhibited PG (mpy) DOWFROST™ LC 25 (mpy)
Copper 0.08 0.16 0.03
Solder 3.14 34.70 0.04
Brass 0.23 0.20 0.07
Mild Steel 9.69 9.80 0.02
Cast Iron 21.20 16.20 0.02
Aluminum 13.20 1.80 0.31

Corrosion performance evaluated using ASTM D1384 testing at 190 °F (88 °C) for two weeks with constant air bubbling. Glycol solutions were prepared at 30 vol%. Corrosion rates are reported as mils penetration per year (mpy). Corrosion rates above 0.5 mpy (2.5 mpy for aluminum) generally indicate insufficient corrosion protection.

For detailed specifications, material properties, and application guidance relevant to direct-to-chip liquid cooling:

FAQ

Frequently Asked Questions About DOWFROST™ LC 25

▶ Is DOWFROST™ LC 25 compatible with elastomers and plastics used in liquid cooling systems?

DOWFROST™ LC 25 is formulated to maintain chemical compatibility with a wide range of elastomers and plastics commonly used in liquid cooling systems operating at bulk fluid temperatures up to 90 °C (194 °F). Compatibility depends on both material type and allowable service temperature, which can vary significantly between different formulations of the same polymer or elastomer.

Materials such as PTFE and FEP exhibit excellent compatibility at elevated temperatures, while EPDM, polyethylene (PE), polypropylene (PP), and polysulfone-based polymers (PSU, PPSU) are generally suitable for operation up to approximately 75 °C.

Some elastomers and plastics, including NBR, silicone, polyamide (PA), polyoxymethylene (POM), and certain fluoroelastomers (FKM), may have lower recommended temperature limits or reduced long-term stability when exposed to propylene glycol–based fluids.

▶ Can DOWFROST™ LC 25 heat transfer fluid be diluted?

DOWFROST™ LC 25 is a ready-to-use heat transfer fluid and should not be diluted. It is formulated with the correct concentration of corrosion inhibitors to protect datacom equipment cooling systems (DECS) and other liquid cooling loops. Dilution lowers inhibitor effectiveness and can increase the risk of corrosion, scaling, and biological fouling.

If dilution is unavoidable, only purified water—distilled, deionized (DI), or reverse osmosis (RO)— should be used. Untreated or mineral-rich water can introduce contaminants that degrade system reliability.

Minimum water quality limits for any unavoidable dilution:

Total Chlorides (as Cl⁻) < 25 mg/L
Total Sulfates (as SO₄²⁻) < 25 mg/L
Total Hardness (as CaCO₃) < 50 mg/L
Total Iron (as Fe) < 1 mg/L
Electrical Conductivity < 50 µmhos/cm
pH 5 < pH < 9
▶ Why does DOWFROST™ LC 25 have higher electrical conductivity than purified water, and is it a concern?

DOWFROST™ LC 25 contains corrosion inhibitors, pH buffers, and stabilizing additives that are intentionally added to protect metals and maintain long-term fluid performance. These additives increase ionic content, resulting in electrical conductivity values typically above 2,000 µmhos/cm. This behavior is normal for a fully formulated heat transfer fluid.

The higher conductivity is not a concern because DOWFROST™ LC 25 is used in closed-loop liquid cooling systems, where the fluid is fully contained and isolated from electronic circuits. Conductivity reflects the chemistry required for corrosion control and system reliability, not electrical risk.

Featured Presentation

Solutions for Data Center Cooling

Related blogs

Further Reading on Direct-to-Chip Cooling

Heat Transfer Fluids for Direct-to-Chip Cooling in Data Centers

Heat Transfer Fluids for Direct-to-Chip Cooling in Data Centers

Rose Anne Acedera, March 2026

This article explains the role of heat transfer fluids in direct-to-chip (D2C) cooling systems used in modern data centers. It discusses key fluid properties such as thermal conductivity, viscosity, electrical resistivity, and long-term stability, helping engineers select suitable coolants for high-power processors and AI workloads.

Support reliable direct-to-chip liquid cooling deployments.

DOWFROST™ LC 25 can be purchased through our parent company, Krayden. Contact us to discuss heat transfer fluid selection, material compatibility, and long-term reliability considerations for high-density data center and AI cooling systems.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers