Hysol GR17 | White Epoxy Mold Compound
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- Reflective compound
- For Optocouplers
- High moldability
Product Description
Hysol GR17 is a white, reflective epoxy molding compound used for optical applications. This silica filled (68%) product has been designed to improve light reflectance and workability for optocouplers also knows as photo-couplers, optical isolators, or opto-isolators.
Hysol GR17 cures with heat and can be used for transfer processes. It has been formulated to provide high moldability, low stress and high adhesion to a variety of substrates. Transmissivity is 18.5.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Chemical Properties
Physical Properties
Thermal Properties
Curing Conditions
Additional Information
Storage
Store product in the unopened container in a dry location. Storage information may be indicated on the product container labeling.
Optimal Storage: 5°C or below, in closed containers. After removal from cold storage, the material MUST be allowed to come to room temperature, in the sealed container, to avoid moisture contamination. The suggested waiting time for a standard 15 kg carton box is 24 hours.