Hysol GR300S | Black Epoxy Mold Compound
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- Low CTE (15 ppm/°C)
- Low stress
- High productivity
Product Description
Hysol GR300S is a black, epoxy molding compound used for optical applications. This partly fused silica filled (77%) product has been designed for optocouplers also knows as photo-couplers, optical isolators, or opto-isolators. It is also used for SMX, SOD, BRG, TO and DIP applications.
Hysol GR300S is a heat curable epoxy with low wire sweep, low stress and a low coefficient of thermal expansion. It has a flammability rating of UL94 V-0.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Chemical Properties
Physical Properties
Thermal Properties
Curing Conditions
Additional Information
Storage
Store product in the unopened container in a dry location. Storage information may be indicated on the product container labeling.
Optimal Storage: 5°C or below, in closed containers. After removal from cold storage, the material MUST be allowed to come to room temperature, in the sealed container, to avoid moisture contamination. The suggested waiting time for a standard 15 kg carton box is 24 hours.