Hysol GR360A-ST | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

GR360A-ST(68C) Black Epoxy Mold Compound GR360A-ST Black Epoxy Mold Compound

Main features

  • Low cost of ownership
  • 77% filler weight
  • For Diodes, TO and DIP

Product Description

Hysol GR360A-ST epoxy molding compound delivers outstanding performance and ease of use. This "Green" environmentally friendly epoxy molding compound contains no bromine, antimony or phosphorus flame retardant. It provides the lowest cost of ownership with superior moldability and reliability.

Hysol GR360A-ST has an 77% filler loading and is typically used for Diodes, TO and DIP packages. It meets UL 94 V-0 Flammability at 6.35mm thickness. Its CTI, comparative tracking index value is 500V.

  • GR360:  CTI = 500 V (PLC-1 / IEC Material Group II)
  • GR360A: CTI = 450 V (PLC-1 / IEC Material Group II)
Product Family

HYSOL GR360A-ST

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
Black
Filler Content Filler Content
77 %
Specific Gravity Specific Gravity
1.84
Chemical Properties
Moisture absorption Moisture absorption
0.49 %
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
168 °C
UL 94 Rating UL 94 Rating
V0
Physical Properties
Spiral Flow @ 175°C Spiral Flow @ 175°C
98 cm
Curing Conditions
Transfer Pressure Transfer Pressure
40 - 100 kg/cm2
Transfer Time Transfer Time
10 - 20 s