Hysol KL1000-3A | Black Epoxy Mold Compound
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- Lowest Cost of Ownership
- Excellent Moldability
- Designed for ZIP, SIL, DIP packages
Product Description
Hysol KL1000-3A is a black, semiconductor grade epoxy molding compound. It provides the lowest cost of ownership for an epoxy molding compound. It works on easy, low-end discrete semiconductor packages for companies that still use halogen-containing epoxy molding compounds.
Hysol KL1000-3A has a history that predates the acquisition of Huawei Electronics by Henkel. In 2005, Henkel formed a joint-venture with HuaweI Electronics in China to create Henkel Huawei Electronics (HHE) in Lianyungang China. HHE made low-end, halogen containing epoxy molding compounds that used Bromine or Antimony as a flame retardant. The KL1000-3A is an old product that is still made at Hysol Huawei today.
Hysol KL1000-3A is a halogen containing, legacy product that has been used for decades with great success for bridge rectifiers, PDIP and low end packages such as Zig zag In line (ZIP), Single In Line (SIL), Dual In line (DIP) and other low end semiconductor discrete Packages.
Packaging
Technical Specifications
General Properties
Chemical Properties
Physical Properties
Thermal Properties
Electrical Properties
Curing Conditions
Additional Information
{tab=Technical Specifications}
Typical applications and uses of {product_name} include:
Technical Datasheets for {product_name}TDS (English) |
{tab=Videos & Other Media}
|
Sorry, there are no related videos at this time. |
{tab=View Blogs & Forum}
|
CAPLINQ is different. Unlike other business to business enterprises, we encourage our customers to discuss, critique and otherwise comment on the products we offer. Get more technical information, read detailed posts, and see what customers have to say about{product_name} on our Corporate Blog and Forum. |
{/tabs}