Hysol MG27F-0521LF | Gold Epoxy Mold Compound
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- UL listed file number E255557
- Long Flow version of MG27F-0521
- Used for ceramic capacitors
Product Description
Hysol MG27F-0521 LF is a specially formulated Gold, laser markable product designed for use in high volume molding of multi-layer ceramic capacitors (MLCC). MG27F-0521 LF was developed to provide optimum moldability in conventional transfer molding applications. It features good moisture resistance and low ionics. Its gold color provides excellent contrast in lasermark applications.
Hysol MG27F-0521 LF is listed under the UL file number E255557. It is a UL listed product for Multi Layer Ceramic Capacitors (MLCC). The entire list of UL-listed products can be found at the Hysol UL-listed Epoxy Molding compounds
Hysol MG27F-0521LF is designed for the following semiconductor packages:
- Multi-Layer Ceramic Capacitors
- Cermaic Resistors
- Other passive electronics components