TC-8020T | Optically Clear Molding Compound
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- LED Encapsulation
- Optically clear
- Emitter and Detector encapsulation
Product Description
OPTOLINQ TC-8020T is a high transmission, one component, optically clear epoxy molding compound that is specifically developed for emitter and LED encapsulation. Its excellent fluidity design aids it to become easily mouldable and processable while offering excellent package performance and durability. This is supported by its long term transmittance and post reflow reliability.
OPTOLINQ TC-8020T is a single component epoxy with superior adhesion performance, transmittance and stability at high temperatures. It is mainly utilised to package single color (monochrome) LEDs, 7-segment LED displays, compact LED indicators, monochrome ChipLEDs and photo-links.It offers good adhesion to Bismaleimide Triazine - BT substrates and metal leadframes, good flexural modulus, and excellent anti-reflow performance while also passing the stringent MSL 3/2A JEDEC requirements. Check TC-8020T Internal Reliability Test Results.
Typical Applications
- Low-Power LED & Emitters
- Pulse Oximeter Sensors
- Ambient Light Sensors
- IR and Near-IR Sensors
- Data transmission and industrial fibers.
Versions Available
- Low-stress versions TC-8020L/LS (DMA modulus comparison)
- Self-release version TC-8020T-SR (Series property comparison)
- Optical filter versions TC-8020T-IR800/840 (Transmittance curve)
Comparable With: XX-18, XX-8524, XX-330H
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Chemical Properties
Curing Conditions
Physical Properties
Additional Information
| PROPERTY | UNIT | TC-8020T | TC-8020L | TC-8020LS | TC-8020T-SR |
| Viscosity | cP | 300 | 300 | 200 | 300 |
| Spiral Flow @150°C | cm | 150-250 | 150-250 | 150-250 | 150-250 |
| Hot Plate Gel Time @150°C | sec | 20-40 | 25-50 | 20-50 | 20-40 |
| Glass Transition Temperature | °C | 125 | 115 | 95 | 125 |
|
CTE by TMA, α1 CTE by TMA, α2 |
ppm ppm |
70 170 |
70 170 |
70 220 |
70 170 |
|
Moisture Absorption PCT 24 hrs @25°C water 24 hrs @121°C, 2atm, 100%RH |
wt% wt% |
0.17 3.2 |
0.16 3.2 |
0.17 3.8 |
0.17 3.2 |
|
Flexural Strength @25°C Flexural Modulus @25°C |
MPa Mpa |
130 3000 |
130 2900 |
110 3100 |
130 3000 |
|
yellowing Δb - 4 hrs @200°C yellowing Δb - 30 min @280°C yellowing Δb - 4 hrs UV |
- |
5 33 11 |
8 42 16.5 |
25 45 16.5 |
5 37 11 |
| Transmittance 1mm @450nm | % | >90 | >90 | >90 | >90 |
| Refractive Index @633nm | - | 1.56 | 1.56 | 1.56 | 1.56 |
| Comment | Standard Item for through-hole and surface mount component | Low stress version for better reflow performance | Low stress for balanced reflow and thermal shock test performance | Self-release technology without compromising key properties |
TC-8020L/LS shows lower modulus at 150℃ and -50℃, which improves performance in thermal cycling and thermal shock tests.
TC-8020T DSC Curve
TC-8020T DMA Data CurveTransmittance wavelength window could be adjusted according to customers' specifications.