TMC-8020LS | Clear Optical Molding Compound
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- LED Encapsulation
- Low stress
- Better reflow and Thermal shock
Product Description
OPTOLINQ TMC-8020-LS is a high-performance optical solid epoxy specifically developed for LED encapsulation. This monocomponent epoxy achieves superior adhesion performance and great transmittance. It has lower Tg than the "normal" 8020 version.
OPTOLINQ TMC-8020-LS is able to offer low blue-ray decay for outdoor LED applications and overall great light performance. This low stress white epoxy is very close to competitive solutions such as XX814, XX1000 and XX97. It is a reliable product that has improved reflow abilities and thermal shock test performance.
Packaging
Technical Specifications
General Properties
Thermal Properties
Chemical Properties
Curing Conditions
Physical Properties
Additional Information
| PROPERTY | UNIT | TMC-8020L | TMC-8020LS |
| Viscosity | cP | 300 | 200 |
| Spiral Flow @150°C | cm | 150-250 | 150-250 |
| Hot Plate Gel Time @150°C | sec | 25-50 | 20-50 |
| Glass Transition Temperature | °C | 115 | 95 |
|
CTE by TMA, α1 CTE by TMA, α2 |
ppm ppm |
70 170 |
70 220 |
|
Moisture Absorption PCT 24 hrs @25°C water 24 hrs @121°C, 2atm, 100%RH |
wt% wt% |
0.16 3.2 |
0.17 3.8 |
|
Flexural Strength @25°C Flexural Modulus @25°C |
MPa Mpa |
130 2900 |
110 3100 |
|
yellowing Δb - 4 hrs @200°C yellowing Δb - 30 min @280°C yellowing Δb - 4 hrs UV |
- |
8 42 16.5 |
25 45 16.5 |
| Transmittance 1mm @450nm | % | >90 | >90 |
| Refractive Index @633nm | - | 1.56 | 1.56 |
| Comment | Low stress version for better reflow performance | Low stress for balanced reflow and thermal shock test performance |