TMC-8040 | Optically clear Molding Compound
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- High reliability
- 7 segment monochrome LED
- Medium blue ray decay
Product Description
OPTOLINQ TMC-8040 is a high-performance optically clear epoxy developed for high reliability white chip monochrome LED applications. This anhydride cured, monocomponent BisA and Cycloaliphatic combination achieves superior adhesion performance and great transmittance. Its stability at high temperature aids towards a good package performance and long life. It works very similar, if better than XX-600H product types.
TMC-8040 is able to offer medium anti-blue-light decay stability. It maintains high blue-wavelength transmittance with minimal yellowing, offers strong moisture resistance, and has shown robust performance in TCT, PCT, and IR-reflow with low discoloration. It is engineered to meet JEDEC MSL 3 / 2A requirements for reliable assembly.
OPTOLINQ TMC-8040 is developed based on TMC-8020T with improved moisture resistance and anti-blue decay properties. Check the Reliability Test Comparison between TMC-8040 and TMC-8020T.
Typical Applications
- Low-Power LED & Emitters
- Pulse Oximeter Sensors
- Ambient Light Sensors
- IR and Near-IR Sensors
- Data transmission and industrial fibers.
Comparable With: XX-600
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Chemical Properties
Curing Conditions
Physical Properties
Additional Information
TMC-8040 exhibits high baseline optical transmission from 400nm to 1000nm - high enough for applications requiring optical clarity
Both TMC-8020 and TMC-8040 pass the reflow tests and double 85 tests, showing no dead lights and no color shift in substrates. TMC-8040 has improved moisture-resistance property, compared with TMC-8020 series and better performance in pressure cooking test (PCT) and blue decay test. TMC-8040 is suitable for surface mount packages, requiring MSL3 & 2A.
| TEST | PRODUCT | TEST CONDITION | RESULT |
| IR Reflow | TMC-8020L | 3 x 30 sec @260°C, IR Reflow | Pass |
| TMC-8040 | 3 x 30 sec @260°C, IR Reflow | Pass | |
| Double 85 Test | TMC-8020L | 5V * 20mA, 75hrs @85°C * 85%RH | Pass |
| TMC-8040 | 5V * 20mA, 75hrs @85°C * 85%RH | Pass | |
Thermal Cycling |
TMC-8020L | -40°C~100°C, 200 cycles | Pass |
| TMC-8040 | -40°C~100°C, 200 cycles | Pass | |
Pressure Cook |
TMC-8020L | 2 x 8hrs @121°C, 100%RH, 2 atm | Fail |
| TMC-8040 | 2 x 8hrs @121°C, 100%RH, 2 atm | Pass |
Yellowing Results Comparison Between TMC-8020L and TMC-8040