LINQSOL EMC-7535 | Black Epoxy Mold Compound
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other
Main features
- Green molding compound
- Designed for high-power TO packages
- High Tg, low water absorption, low modulus, and excellent thermal stability
Product Description
LINQSOL EMC-7535 is a green epoxy molding compound specifically developed for high-voltage and high-power semiconductor devices. It offers low modulus to meet low-stress requirements. With a high glass transition temperature (Tg = 175 °C), minimal moisture absorption, a high comparative tracking index (CTI = 600 V), and a UL 94 V-0 flammability rating, EMC-7535 guarantees strong performance and outstanding reliability.
Overall, LINQSOL EMC-7535 seamlessly integrates advanced material properties, safety compliance, and superior performance, precisely meeting the stringent demands of high-power semiconductor components such as TO packages.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Electrical Properties
Chemical Properties
Physical Properties
Thermal Properties
Mechanical Properties
Curing Conditions
Additional Information
Processing Instructions
- Before use, let LINQSOL EMC-7535 reach room temperature for 24 hours. Keep the bag unopened and stored in a dry location with a relative humidity of ≤50% during thawing to prevent moisture contamination.
- Use the materials within 72 hours after removing the container from cold storage.
Storage and Handling
LINQSOL EMC-7535 is available in pressed pellets in a wide range of sizes to meet specific customer needs. To ensure product integrity, keep it away from oxidizing materials. For long-term storage, maintain a cold environment. The shelf life at 5 °C is 183 days.