Molykote

MOLYKOTE

MOLYKOTE Specialty Lubricants & Lubrication Solutions

MOLYKOTE® is DuPont's specialty-lubricants portfolio for controlling friction, wear, sealing, release, and component movement across automotive and industrial equipment. The portfolio spans greases, oils & fluids, pastes, compounds, anti-friction coatings, and dispersions, with product technologies that include mineral oil, synthetic hydrocarbon, ester, silicone, fluorosilicone, PFPE, and solid-lubricant systems. Depending on the product, MOLYKOTE solutions support bearings, gears, chains, compressors, pumps, valves, seals, threaded connections, electric motors, sliding surfaces, and other demanding lubrication points.

As an authorized MOLYKOTE distributor, Krayden supplies specialty lubricants for equipment design, production, maintenance, and repair applications. Our team can help compare lubricant type, base chemistry, viscosity or consistency, load, speed, temperature, environmental exposure, material compatibility, and application method so customers can narrow the appropriate MOLYKOTE options for a specific operating condition.

Markets Served by MOLYKOTE

Automotive Aerospace Chemical & Petrochemical Energy & Utilities Facilities & Infrastructure Food & Beverage Heavy Industries Home Appliances & Equipment Industrial MRO Oil & Gas Water Management
 
MOLYKOTE grease lubrication application
MOLYKOTE® Grease Lubrication

Greases

MOLYKOTE greases combine a lubricating fluid, thickener, and performance additives or solid lubricants to stay in place where a flowing oil is not practical. The portfolio spans general machinery lubrication, high-load and severe-duty service, wide-temperature applications, chemically demanding environments, and low-noise or precision-bearing duties. Selection should account for load, environment, temperature, speed, relubrication interval, base-oil chemistry, thickener system, and compatibility with nearby metals, plastics, elastomers, or process media.

MOLYKOTE BR-2 High Performance Grease
Application Class

General & Heavy-Duty Greases

Mineral- and synthetic-oil greases for bearings, gears, slides, drives, and other machinery where staying power, wear protection, corrosion resistance, or load-carrying performance may be required. Confirm the exact product's speed, temperature, material-compatibility, and relubrication requirements.

MOLYKOTE extreme-environment grease
Base Chemistry

Extreme-Environment & Chemical-Resistant Greases

Specialty MOLYKOTE greases are considered for high-temperature, chemically demanding, reactive, or otherwise severe environments where conventional lubricants may not be appropriate. Product-specific compatibility with gases, chemicals, elastomers, metals, and process conditions must be confirmed.

MOLYKOTE electric motor and precision bearing grease
Application Class

Electric-Motor & Precision-Bearing Greases

Greases for electric motors and precision rotating equipment are selected around bearing type, speed, noise targets, temperature, load, and service interval. Selected MOLYKOTE formulations also address applications involving engineered plastics or mixed-material assemblies.

 
MOLYKOTE oils and fluids lubrication application
MOLYKOTE® Fluid Lubrication

Oils & Fluids

MOLYKOTE oils and fluids provide flowing lubrication for gears, gearboxes, pumps, chains, compressors, vacuum equipment, slides, and other machinery where circulation, penetration, or controlled fluid delivery is preferred over a grease. The portfolio includes mineral and synthetic base-fluid technologies. Selection should consider viscosity, operating temperature, load and speed, oxidation or corrosion exposure, equipment design, material compatibility, and any process-specific requirements.

MOLYKOTE gear and gearbox oil
Application

Gear, Gearbox & Pump Oils

Fluid lubricants for enclosed gears, gearboxes, and pump-related machinery can be selected around viscosity, gear or bearing geometry, load, speed, temperature, oxidation stability, corrosion protection, and equipment-material compatibility.

MOLYKOTE compressor and vacuum pump oil
Application

Compressor & Vacuum Pump Oils

Compressor and vacuum-service oils are chosen for the exact equipment design, gas or process environment, temperature, volatility requirements, deposit control, corrosion exposure, and compatibility with seals and other wetted materials.

MOLYKOTE chain and multipurpose lubrication fluid
Application

Chain, Slide & Multipurpose Fluids

Flowing lubricants and penetrant-type fluids can support chains, sliding surfaces, guides, tracks, and other points that benefit from liquid delivery. Selection depends on penetration, retention, temperature, speed, contamination exposure, and the equipment's required lubrication method.

 
MOLYKOTE assembly paste application
MOLYKOTE® Assembly & Anti-Seize Lubricants

Pastes

MOLYKOTE pastes are greaselike lubricants with a high concentration of solid lubricants for assembly, running-in, anti-seize, and heavily loaded metal contact. They are commonly considered for threaded connections, press fits, splines, gears, and other slow-moving or startup contacts where the carrier oil may be displaced but a solid lubricating film is still needed. Product selection should consider substrate metallurgy, load, temperature, corrosion exposure, required friction behavior, and assembly or disassembly requirements.

MOLYKOTE anti-seize paste
Application

Threaded Connections & Anti-Seize

Anti-seize and assembly pastes help control friction and reduce seizure or galling risk on threaded fasteners and other metal-to-metal connections. The correct paste depends on alloy, service temperature, load, corrosion environment, tightening method, and whether later nondestructive disassembly is required.

MOLYKOTE G-N Metal Assembly Paste
Application

Assembly & Running-In Pastes

Running-in and assembly pastes are used on press fits, splines, gears, bearings, and other highly loaded contacts during installation or startup. They provide solid-lubricant coverage at low speed or during initial movement before the normal operating lubricant establishes a full film.

 
MOLYKOTE silicone compound application
MOLYKOTE® Silicone Compounds

Compounds

MOLYKOTE compounds are greaselike silicone-based materials used where lubrication and sealing, release, electrical insulation, moisture resistance, or compatibility with rubber and plastics may be required. The category extends beyond release compounds to include valve and seal lubrication, O-ring assembly, dielectric moisture barriers, noncuring sealing functions, and selected plastic or elastomer lubrication duties. Confirm product-specific compatibility and any regulatory or process requirements for the intended application.

MOLYKOTE seal and O-ring lubricating compound
Function

Seal, O-Ring & Dielectric Compounds

Selected MOLYKOTE compounds are used as lubricants or sealants for valves, packings, seals, and O-rings, while other products serve as nonconductive dielectric or moisture-barrier compounds for electrical equipment. The intended material pair and service medium are important selection inputs.

MOLYKOTE 7 Release Compound
Function

Release & Plastic/Rubber Lubrication Compounds

Release compounds remain an important part of the MOLYKOTE compound portfolio for molds and other anti-stick duties. Selected compounds also support lubrication of plastic, rubber, elastomer, cable, and sliding interfaces where the specified product is compatible with the materials in contact.

 
MOLYKOTE anti-friction coating application
MOLYKOTE® Dry-Film Lubrication

Anti-Friction Coatings

MOLYKOTE anti-friction coatings are bonded dry-film lubricants containing solid lubricants dispersed in resin and solvent systems. After application and curing, they form a thin lubricating film on the component surface and are used where a clean, dry lubricant is preferred, where dust or contamination makes wet lubrication undesirable, or where relubrication access is limited. Coating choice depends on substrate, surface preparation, application method, cure requirements, film thickness, load, motion, and service environment.

MOLYKOTE D-321 R Anti-Friction Coating
Coating Type

Bonded Dry-Film Coatings

Bonded coatings use solid lubricants held in a resin matrix to create a dry lubricating surface after cure. They can be considered for sliding contacts, intermittent motion, dusty environments, and components that are difficult to service with oils or greases.

MOLYKOTE 106 Anti-Friction Coating
Coating Type

General Anti-Friction Coatings

MOLYKOTE offers multiple anti-friction coating formulations for dry-film lubrication of metals and, depending on the product, selected plastics or elastomers. The binder and solid-lubricant system influence cure, adhesion, friction behavior, wear life, and service-temperature capability.

 
MOLYKOTE dispersion lubrication application
MOLYKOTE® Solid Lubricants in Liquid Form

Dispersions

MOLYKOTE dispersions suspend finely divided solid lubricants in a liquid carrier so the lubricant can be applied by liquid methods, including automatic dispensing where appropriate. They are used for dry-film lubrication of sliding contacts, lubrication of chains, conveyors and bearings in demanding temperature conditions, selected cutting or sewing operations, release applications, and other specialty processes. Selection should consider carrier chemistry, evaporation or residue behavior, application equipment, surface material, required film, temperature, and process compatibility.

MOLYKOTE solid lubricant dispersion
Application Method

Dry-Film & Sliding-Contact Dispersions

Dispersions can deliver solid lubricants to sliding contacts and other surfaces in a liquid-applied form, including processes where a thin residual lubricating film is preferred. Automatic application may be practical for selected products and production methods.

MOLYKOTE chain and release dispersion
Application

Chain, Release & Process Dispersions

Other MOLYKOTE dispersions support chains, conveyors, bearings, release duties, and selected cutting or sewing processes where a liquid carrier provides convenient access to the lubrication point. The correct formulation depends on the process, temperature, contamination limits, and desired surface residue.

Talk to our Experts

Whether you are comparing a grease, oil, paste, compound, coating, or dispersion, Krayden can help narrow MOLYKOTE options around the actual lubrication point. Our team can support product comparison, application requirements, load-speed-temperature review, material compatibility, environmental exposure, and practical application or maintenance considerations.

Contact our team Call +1 (800) 448-0406

MOLYKOTE Quick Reference

Brands Carried
MOLYKOTE
Core Technology
Specialty Lubricants & Solid Lubrication
Top Categories
Greases, Oils & Fluids, Pastes
Key Markets
Automotive, Aerospace, Industrial MRO, Energy & Utilities

129 products

  • MOLYKOTE 3451 Chemical Resistant Bearing Grease

    MOLYKOTE 3451 Chemical Resistant Bearing Grease

    • Fluorosilicone Grease Formulation
    • 40 to 450 deg F Service Range
    • 340 kg Four-Ball Weld Load
  • MOLYKOTE 7 RELEASE COMPOUND

    MOLYKOTE 7 RELEASE COMPOUND

    • 40 to 204 deg C Service Range
    • Release, Lubrication, Sealing, and Protection
    • 0.8% Evaporation at 200 deg C
  • MOLYKOTE D-321R AN-FR

    MOLYKOTE D-321R AN-FR

    • Room-Temperature Application Cure
    • Dry Film Lubricant Formulation
    • 180 to 450 deg C Service Range
  • MOLYKOTE EM-D110 GREASE

    MOLYKOTE EM-D110 GREASE

    • Compatible with Most Plastics
    • High-Viscosity PAO Oil
    • Silicone-Free Lubrication Formulation
  • MOLYKOTE G-2008 Synthetic Tool Gear Grease

    MOLYKOTE G-2008 Synthetic Tool Gear Grease

    • Fully Synthetic PAO-Based Grease with Lithium Thickener
    • Manual or Automated Dispensing
    • Sub-0.55 mm Four-Ball Wear
  • MOLYKOTE G-68 Plastic Gear Grease

    MOLYKOTE G-68 Plastic Gear Grease

    • Good Compatibility with Most Plastics
    • 0.014 Coefficient of Friction
    • Water-Resistant Grease Lubrication
  • MOLYKOTE G-N METAL ASSEMBLY PASTE

    MOLYKOTE G-N METAL ASSEMBLY PASTE

    • Heavy-Duty Assembly Paste
    • 0.08 Coefficient of Friction
    • Metal Interfaces Protection
  • MOLYKOTE HI-VAC SILICONE BASED HIGH VACUUM GREASE

    MOLYKOTE HI-VAC SILICONE BASED HIGH VACUUM GREASE

    • Low-Volatility Silicone Grease
    • Less Than 0.5% Bleed
    • Seals and Lubricates Vacuum and Pressure Systems
  • DUROPTIX OE-6370

    DUROPTIX OE-6370

    • 1:1 Optical Encapsulant Mixing
    • 100% Transparent Optical Protection
    • 240-Minute 150 deg C Cure
  • DUROPTIX OE-6550

    DUROPTIX OE-6550

    • 1:1 Controlled Mixing
    • High Optical Transmittance
    • High Refractive Index
  • ECCOSORB AN-77

    ECCOSORB AN-77

    • Carbon Loaded, Multilayer Absorber
    • Broadband Free Space Absorber
    • Low-Weight RF Absorber
  • LAIRD GDS

    LAIRD ECCOSORB GDS

    • Thin Conformable Construction
    • High-Frequency RF Attenuation
  • LAIRD JCP-PP9

    LAIRD JCP-PP9

    • 60+ GHz Injection-Moldable Absorber
    • 76 to 81 GHz Automotive Radar Use
    • Polypropylene-Like Mechanical Integration
  • LAIRD LS-26

    LAIRD LS-26

    • High-Loss Microwave Absorption
    • Low-Density Urethane Foam
    • Very Flexible Absorber Foam
  • LAIRD MCS/SS6M

    LAIRD MCS/SS6M

    • 800 MHz to 6 GHz Absorption
    • Low-Outgassing Silicone Construction
    • Flexible Sheet with Optional PSA
  • LAIRD TPUTTY 502FG2

    LAIRD TPUTTY 502FG2

    • 3.0 W/(m K) Thermal Interface
    • Ultra-Soft 14 Shore 00 Material
    • Thermal Interface Material
  • LAIRD VY-81

    LAIRD VY-81

    • 80 to 90 dB EMI/RF Shielding
    • Non-Hardening High-Tack Shielding Compound
    • Conventional Caulking-Equipment Application
  • MOLYKOTE 1000

    MOLYKOTE 1000

    • No Intentional PFAS, Lead, or Nickel
    • -30 to 650 deg C Service Range
    • Consistent Friction and High Load Capacity
  • MOLYKOTE 106

    MOLYKOTE 106

    • Heat-Curing Dry Film Lubricant
    • High-Load Coating Application
    • 70 to 250 deg C Service Range
  • MOLYKOTE 112

    MOLYKOTE 112

    • Up to 232 deg C Service
    • Oil, Acid, and Alkali Resistance
    • Low-Volatility Joint Sealing
  • MOLYKOTE 1122

    MOLYKOTE 1122

    • High-Viscosity Lubricant Formulation
    • Robust High-Pressure Resistance and Wear Protection
    • High-Temperature Lubrication Protection
  • MOLYKOTE 3099

    MOLYKOTE 3099

    • Water-Repellent High-Voltage Insulator Coating
    • 800-Minute ASTM D2303 Arc Resistance
    • Hand, Pad, Brush, or Spray Renewal
  • MOLYKOTE 316

    MOLYKOTE 316

    • Effective, Heat-Stable Anti-Stick Silicone Film
    • FDA 21 CFR 175.300 Compliance
    • Oxidative Breakdown Resistance
  • MOLYKOTE 3179

    MOLYKOTE 3179

    • Dilatant Rheological Behavior
    • Non-Slumping Static-Flow Resistance
    • Novelty/Educational Toy-Market Use
  • MOLYKOTE 33

    MOLYKOTE 33

    • NLGI 2 Silicone Grease
    • Water-Resistant Light-Load Lubrication
    • 73 to 180 deg C Service Range
  • MOLYKOTE 3400A

    MOLYKOTE 3400A

    • 30-Minute 200 deg C Heat Cure
    • High-Load Dry-Film Wear Resistance
    • 500-Hour Red-Rust Resistance
  • MOLYKOTE 3452

    MOLYKOTE 3452

    • Multi-Solvent Chemical Resistance
    • Defined 8-Hour Exposure Testing
    • 400 kg Four-Ball Weld Load
  • MOLYKOTE 4

    MOLYKOTE 4

    • 54 to 200 deg C Service Range
    • 3 ohm-cm Volume Resistivity
    • Flowable Controlled Placement
  • MOLYKOTE 41

    MOLYKOTE 41

    • Silicone Oil Base and Carbon Black Thickener
    • 20 to 290 deg C Service Range
    • Water and Oxidation Resistance
  • MOLYKOTE 44

    MOLYKOTE 44

    • -40 to 200 deg C Service Range
    • 2.5% Bleed at 150 deg C
    • NLGI 2-3 Silicone Grease
  • MOLYKOTE 5

    MOLYKOTE 5

    • Nonconductive, Water-Repellent Silicone Paste
    • 54 to 232 deg C Service Range
    • Metal and Plastic Compatibility
  • MOLYKOTE 55

    MOLYKOTE 55

    • Silicone Base Oil and Lithium Soap Thickener
    • Heat-Stable Oxidation-Resistant Grease
    • D4/D5/D6 Cyclic-Siloxane Compliance
  • MOLYKOTE 557

    MOLYKOTE 557

    • Clear Nonstaining Wax-Like Film
    • 0.07 Coefficient of Friction
    • Federal Meat/Poultry Program Authorization
  • MOLYKOTE 7400

    MOLYKOTE 7400

    • Water-Based MoS2/Graphite Dry-Film Lubricant
    • High Load-Carrying Capacity
    • Air-Curing Lubricant Coating
  • MOLYKOTE 7415

    MOLYKOTE 7415

    • Molykote D-7405, D-7409, and D-7620 Anti-Friction Coatings
    • Low Evaporation Rate
    • PTFE- and PFAS-Free Formulation
  • MOLYKOTE BG20

    MOLYKOTE BG20

    • 45 to 180 deg C Service Range
    • 2,400 N Four-Ball Weld Load
    • Manual or Automated Dispensing
  • MOLYKOTE BG-555

    MOLYKOTE BG-555

    • Low-Noise Bearing Grease
    • Water-Washout and Corrosion Resistance
    • -40 to 150 deg C Service Range
  • MOLYKOTE BR-2

    MOLYKOTE BR-2

    • MoS2/Graphite Lithium Grease
    • High-Load Moderate/High-Speed Lubrication
    • Long-Term Industrial Lubrication
  • MOLYKOTE CU-7439

    MOLYKOTE CU-7439

    • Up to 650 deg C Service
    • High-Adhesion Copper Paste
    • Nondestructive Thread-Disassembly Support
  • MOLYKOTE D-10-GBL

    MOLYKOTE D-10-GBL

    • 15 to 20 um Dry Film
    • -40 to 340 deg C Service Range
    • 5,500 N Falex Load
  • MOLYKOTE D-321

    MOLYKOTE D-321

    • 5-Minute Cure Cycle
    • 180 to 450 deg C Service Range
    • 12,500 N Falex Load
  • MOLYKOTE D-708

    MOLYKOTE D-708

    • 700-Hour Cure Cycle
    • 60 to 240 deg C Service Range
    • 60-Minute 180 deg C Cure
  • MOLYKOTE D-7409

    MOLYKOTE D-7409

    • Heat-Curing Dry-Film Lubricant
    • High-Load Wear-Resistant Dry-Film Lubrication
    • Solvent and Oil Resistance
  • MOLYKOTE D-96

    MOLYKOTE D-96

    • Transparent Water-Based PTFE Dry Film
    • 100,000-Cycle No-Noise Pairing Result
    • -40 to 150 deg C Service Range
  • MOLYKOTE DX

    MOLYKOTE DX

    • 4,800 N Four-Ball Weld Load
    • 0.10 Press-Fit Friction Coefficient
    • -25 to 125 deg C Service Range
  • MOLYKOTE EM-30L

    MOLYKOTE EM-30L

    • -45 to 150 deg C Service Range
    • 3,730 N Four-Ball Weld Load
    • 0.4% Evaporation at 99 deg C
  • MOLYKOTE EM-50L

    MOLYKOTE EM-50L

    • Broad Plastic Compatibility
    • 100% Silicone-Free PAO Grease
    • Low-Seepage Long-Service Lubrication
  • MOLYKOTE E-PASTE

    MOLYKOTE E-PASTE

    • 560 kg Four-Ball OK Load
    • ABS, Polycarbonate, Nylon, Polyacetal Compatibility
    • -50 to 150 deg C Service Range
  • MOLYKOTE G-0010

    MOLYKOTE G-0010

    • Polyurea-Thickened Mineral-Oil Grease
    • Above 260 deg C Dropping Point
    • Corrosion-Preventive Bearing Grease
  • MOLYKOTE G-0050

    MOLYKOTE G-0050

    • FDA 21 CFR 178.3570 Compliance
    • 3,922 N Four-Ball Weld Load
    • Clean, White Color
  • MOLYKOTE G-0052

    MOLYKOTE G-0052

    • FDA 21 CFR 178.3570 Compliance
    • 6,080 N Four-Ball Weld Load
    • Water-Resistant Grease Lubrication
  • MOLYKOTE G-1033

    MOLYKOTE G-1033

    • FDA 21 CFR 178.3570 Compliance
    • 3,922 N Four-Ball Weld Load
    • Clean, White Color
  • MOLYKOTE G-1067

    MOLYKOTE G-1067

    • Low-Friction Plastic-Compatible PAO Grease
    • 50 to 120 deg C Service Range
    • Automotive Lubrication Applications
  • MOLYKOTE G-1502FM

    MOLYKOTE G-1502FM

    • Oil and Water Resistance
    • FDA 21 CFR 178.3570 Compliance
    • 40 to 149 deg C Service Range
  • MOLYKOTE G-3000

    MOLYKOTE G-3000

    • Dual-Mass-Flywheel High-Shear Grease
    • -40 to 180 deg C Service Range
    • 2,200 N Four-Ball Weld Load
  • MOLYKOTE G-3407

    MOLYKOTE G-3407

    • -40 to 200 deg C Service Range
    • Brake-Caliper Guide-Pin Lubrication
    • 120-Hour No-Rust Test Result
  • MOLYKOTE G-4500FM

    MOLYKOTE G-4500FM

    • 40 to 150 deg C Service Range
    • 18 kg Four-Ball Weld Load
    • NLGI 2 PAO/Aluminum-Complex Grease
  • MOLYKOTE G-4501

    MOLYKOTE G-4501

    • FDA 21 CFR 178.3570 Compliance
    • Lower-Consistency (NLGI 1) PAO Synthetic Grease
    • 40 to 150 deg C Service Range
  • MOLYKOTE G-4700

    MOLYKOTE G-4700

    • Extreme-Load Bearing Lubrication
    • PAO Synthetic Base Oil and Lithium Complex Thickener
    • Industrial Plastic/Elastomer Compatibility
  • MOLYKOTE G-5008

    MOLYKOTE G-5008

    • 350 V/mil Dielectric Strength
    • 2.0% Bleed at 204 deg C
    • NLGI 2-3 Silicone/PTFE Grease
  • MOLYKOTE G-5042

    MOLYKOTE G-5042

    • Effective Purple Silicone Grease
    • Siloxane Base Oil and Lithium Soap Thickener
    • Long-Term Silicone-Grease Lubrication
  • MOLYKOTE GN

    MOLYKOTE GN

    • Mineral-Oil Solid-Lubricant Assembly Paste
    • 0.08 Press-Fit Friction Coefficient
    • 2,800 N Four-Ball Weld Load
  • MOLYKOTE HP-300

    MOLYKOTE HP-300

    • Fully Fluorinated PFPE/PTFE Lubrication
    • 65 to 250 deg C Service Range
    • 3,300 N Four-Ball Weld Load
  • MOLYKOTE HP-870

    MOLYKOTE HP-870

    • Fully Fluorinated Formulation
    • -20 to 250 deg C Service Range
    • Chemical-Resistant PFPE/PTFE Grease
  • MOLYKOTE L-1268

    MOLYKOTE L-1268

    • Fully Synthetic ISO Vg 68 PAO Lubrication
    • 54 deg C Pour Point
    • Longer Oil-Drain Intervals
  • MOLYKOTE L13

    MOLYKOTE L13

    • Adjusts the Application Viscosity
    • Compatible Cleaning Solvent
    • Defined Range of Molykote Coatings
  • MOLYKOTE L-1468 FM

    MOLYKOTE L-1468 FM

    • ISO VG 68 PAO Chain Oil
    • Freezer-Chain Anti-Wear Lubrication
    • NSF H1 Registration
  • MOLYKOTE L-1668FM

    MOLYKOTE L-1668FM

    • ISO Vg 68 Mineral-Oil
    • Low Vapor Pressure
    • Carries NSF H1 Certification
  • MOLYKOTE LONGTERM 2 PLUS

    MOLYKOTE LONGTERM 2 PLUS

    • 3,800 N Four-Ball Weld Load
    • Heavily Loaded Metal-to-Metal Components Protection
    • 25 to 110 deg C Service Range
  • MOLYKOTE M-77

    MOLYKOTE M-77

    • Up to 400 deg C Service
    • Silicone Carrier Oil
    • Selected Metal, Plastic, Rubber, and Elastomer Contacts
  • MOLYKOTE P37

    MOLYKOTE P37

    • -30 to 1400 deg C Threaded-Connection Lubrication
    • 5,500 N Four-Ball Weld Load
    • Graphite/Zirconium-Dioxide High-Purity Paste
  • MOLYKOTE P-40

    MOLYKOTE P-40

    • Metal-Free Lubrication Paste
    • Assembly and Continuous Lubrication
    • -40 to 121 deg C Paste Service
  • MOLYKOTE PA-744

    MOLYKOTE PA-744

    • 10 to 20 um Screen-Printed Film
    • High-Wear High-Load Dry Lubrication
    • -75 to 300 deg C Service Range
  • MOLYKOTE PG54

    MOLYKOTE PG54

    • Long-Term Lubrication for Metal-to-Plastic
    • 50 to 180 deg C Service Range
    • Silicone Base Oil
  • MOLYKOTE TP-42

    MOLYKOTE TP-42

    • 3,000 N Four-Ball Weld Load
    • Water-Resistant Grease Lubrication
    • Stick-Slip, Galling, and Corrosion Protection
  • MOLYKOTE YM103

    MOLYKOTE YM103

    • PAO/PTFE Lubrication for Plastic-on-Plastic
    • 45 to 150 deg C Service Range
    • Automotive Lubrication Applications
  • MOLYKOTE Z-POWDER

    MOLYKOTE Z-POWDER

    • 98% MoS2 Solid Lubricant
    • 185 to 400 deg C Service Range
    • 0.048 Coefficient of Friction
  • LAIRD LS-30

    LAIRD LS-30

    • Compliant Polyurethane Foam Format
    • RF Isolation and Insertion Loss
    • Cavity Resonance Suppression
  • LAIRD MF-117

    LAIRD MF-117

    • Machinable RF Component Stock
    • 2.8 to 119 dB/cm Attenuation
    • Sheets, Rods and Bars
  • LAIRD PP-4

    LAIRD PP-4

    • 1.06 Low-Loss Dielectric Constant
    • 0.0001 Loss Tangent
    • Heat-Sealable Closed-Cell Foam
  • LAIRD RFLB/SS6M

    LAIRD RFLB/SS6M

    • Adhesive-Backed 0.51 mm Sheet
    • 10 MHz to 4 GHz Control
    • Greater Than 50 dB/cm Attenuation
  • MOLYKOTE BG-20

    MOLYKOTE BG-20

    • DN 750,000 High-Speed Operation
    • Medium-to-Heavy Load Lubrication
    • -45 to 180 deg C Service
  • MOLYKOTE G-1023

    MOLYKOTE G-1023

    • Steel/GFRP Friction Control
    • -45 to 120 deg C Service
    • Automatic Dispensing Compatible
  • MOLYKOTE G2008

    MOLYKOTE G2008

    • High-Speed Gear Lubrication
    • 30 cSt Synthetic Base Oil
    • -40 to 130 deg C Service
  • MOLYKOTE G684OZTUBES

    MOLYKOTE G684OZTUBES

    • Plastic Gear Friction Control
    • 75 mm2/s Base Oil
    • Brush-to-Central System Application
  • MOLYKOTE P-1042

    MOLYKOTE P-1042

    • 9,000 N Weld Load
    • Water-Emulsion Washout Resistance
    • High-Tack Metal Surface Adhesion
  • MOLYKOTE P-1900

    MOLYKOTE P-1900

    • 3,200 N Weld Load
    • Controlled 0.10 Bolt Friction
    • -30 to 300 deg C Service
  • MOLYKOTE P-3700

    MOLYKOTE P-3700

    • High-Purity Solid-Lubricant Paste
    • 3,000 N Weld Load
    • Controlled M12 Fastener Friction
  • MOLYKOTE P-74

    MOLYKOTE P-74

    • Metal-Free Anti-Seize Formulation
    • 4,800 N Weld Load
    • Controlled M12 Fastener Friction
  • LAIRD BSR

    LAIRD BSR

    • 6-18 GHz cavity-resonance control
    • Flexible, electrically non-conductive silicone construction
    • 0.47% TML / 0.28% CVCM outgassing values
  • LAIRD CF500

    LAIRD CF500

    • X/Y/Z-axis conductive foam for EMI shielding and grounding
    • Low-compression gasket design with a typical 25-50% operating compression range
    • One-sided conductive PSA with die-cut, hole-punch, and notch customization
  • LAIRD CF600

    LAIRD CF600

    • X/Y/Z-axis conductive foam for EMI shielding and grounding
    • Low-compression gasket design with a typical 25-50% operating compression range
    • One-sided conductive PSA with die-cut, hole-punch, and notch customization
  • LAIRD TPUTTY 403

    LAIRD TPUTTY 403

    • 2.3 W/(m K) One-Part Putty
    • 0.05 mm Minimum Bondline
    • ASTM E595 0.05% TML/0.02% CVCM
  • LAIRD TPUTTY SF560

    LAIRD TPUTTY SF560

    • 5.6 W/m-K Non-Silicone Putty
    • 60 g/min Cartridge Flow
    • Low-Fogging Reworkable Interface
  • LAIRD TPCM7125

    LAIRD TPCM7125

    • 0.125 mm Phase-Change Film
    • 7.5 W/m-K Bulk Conductivity
    • 25 Micrometer Minimum Bondline
  • LAIRD TPCM780SP

    LAIRD TPCM780SP

    • Screen-Printable Non-Silicone Paste
    • 5.4 W/m-K Dry-State Conductivity
    • 25 Micrometer Minimum Bondline
  • LAIRD TPCM5200

    LAIRD TPCM5200

    • 0.200 mm Phase-Change Film
    • 5.3 W/m-K Bulk Conductivity
    • 25 Micrometer Minimum Bondline
  • LAIRD SNL60RXP

    LAIRD SNL60RXP

    • 100 dB 200 MHz to 10 GHz Shielding
    • 1-Hour Room-Temperature Handling
    • -50 to 125 deg C Service Range
  • LAIRD TFLEX 3130

    LAIRD TFLEX 3130

    • 3.25 mm Tflex 300 Gap Filler
    • Greater Than 50% Deflection at 50 psi
    • 1.2 W/(m K) Thermal Conductivity
  • LAIRD TFLEX 300

    LAIRD TFLEX 300

    • Over 50% Deflection at 50 psi
    • 1.2 W/(m K) Thermal Conductivity
    • 0.50 to 5.08 mm Thickness Range
  • LAIRD TFLEX 360

    LAIRD TFLEX 360

    • 1.50 mm Gap-Filling Solution
    • 50% Deflection at 50 psi
    • 1.2 W/(m K) Thermal Interface
  • LAIRD TFLEX 640

    LAIRD TFLEX 640

    • 1.02 mm Thickness of Tflex 600 Series
    • 3.0 W/(m K) Thermal Interface
    • Naturally Tacky Surfaces
  • LAIRD TFLEX 6150

    LAIRD TFLEX 6150

    • 3.75 mm Thickness of Tflex 600 Series
    • 3.0 W/(m K) Thermal Interface
    • Naturally Tacky Surfaces
  • LAIRD TFLEX 680

    LAIRD TFLEX 680

    • 2.03 mm Thickness of Tflex 600 Series
    • 3.0 W/(m K) Thermal Interface
    • Naturally Tacky Pad Surfaces
  • LAIRD TFLEX 660

    LAIRD TFLEX 660

    • 1.50 mm Medium-Gap of Tflex 600 Series
    • 3.0 W/(m K) Thermal Interface
    • Easy Assembly and Placement with Naturally Tacky
  • LAIRD TFLEX HD90500

    LAIRD TFLEX HD90500

    • 7.5 W/(m K) Thermal Interface
    • Compliant Silicone Gap Filler
    • Naturally Tacky Construction
  • LAIRD TFLEX HD91000

    LAIRD TFLEX HD91000

    • 1.00 mm Controlled-Compression Pad
    • 7.5 W/mK Thermal Conductivity
    • 0.20 C-in2/W at 10 psi
  • LAIRD TFLEX HD93500

    LAIRD TFLEX HD93500

    • 7.5 W/(m K) Thermal Interface
    • Compliant Silicone Gap Filler
    • Naturally Tacky Construction
  • LAIRD TGON 805

    LAIRD TGON 805

    • 0.13 mm Flexible Graphite Interface
    • 5 W/(m K) Through-Plane Conductivity
    • 0.07 deg C in^2/W Thermal Resistance
  • LAIRD TFLEX 340H
  • LAIRD TFLEX 6110

    LAIRD TFLEX 6110

    • 3 W/mK Thermal Conductivity
    • Greater Than 90% Recovery
    • Naturally Tacky Adhesive-Free Placement
  • LAIRD TFLEX 320H

    LAIRD TFLEX 320H

    • Dry Preformed Interface Pad
    • No Mixing or Dispensing
    • Controlled-Compression Gap Filling
  • LAIRD TFLEX 3200

    LAIRD TFLEX 3200

    • Low-Pressure Compliant Gap Filling
    • Tgard Dielectric Handling Layer
    • Reusable Low-Compression-Set Pad
  • LAIRD TFLEX SF10.0.50

    LAIRD TFLEX SF10.0.50

    • 0.50 mm Thin-Gap Format
    • 10.2 W/m-K Thermal Conductivity
    • Non-Silicone Electrical Insulation
  • LAIRD TFLEX SF10

    LAIRD TFLEX SF10

    • 10 W/m-K Non-Silicone Interface
    • Low-Pressure Thermal Contact
    • 0.3 to 5.0 mm Sheet Range
  • LAIRD TFLEX HP34

    LAIRD TFLEX HP34

    • 34 W/m-K Bulk Conductivity
    • Low Contact Resistance Under Pressure
    • Non-Silicone Aligned-Graphite Construction
  • LAIRD TFLEX HD92000

    LAIRD TFLEX HD92000

    • 2.00 mm High-Deflection Interface
    • 7.5 W/mK Heat Transfer
    • 82% Deflection at 50 psi
  • LAIRD TFLEX HD93000

    LAIRD TFLEX HD93000

    • 3.00 mm High-Deflection Pad
    • 7.5 W/mK Thermal Conductivity
    • Low-Outgassing Silicone Interface
  • LAIRD TPUTTY 506

    LAIRD TPUTTY 506

    • No-Cure Single-Part Putty
    • 3.5 W/m-K Thermal Conductivity
    • Low-Pressure Uneven-Gap Filling
  • LAIRD TPLI2200

    LAIRD TPLI2200

    • 5.08 mm Large-Gap Pad
    • A0 Adhesive-Free Surface
    • 6.0 W/m-K Insulating Interface
  • LAIRD CFS-8480

    LAIRD CFS-8480

    • Broad RF Absorption Capability
    • Flexible Castable Processing
    • Elevated-Temperature Electrical Performance
  • LAIRD CR-110

    LAIRD CR-110

    • Above 26 GHz Absorption Range
    • 100:16.5 Controlled Mixing
    • Below 180 deg C Service Temperature
  • LAIRD CR-114

    LAIRD CR-114

    • 10 to 14 GHz Absorption Range
    • 100:6.5 Controlled Mixing
    • Below 180 deg C Service Temperature
  • LAIRD CR-116

    LAIRD CR-116

    • 6 to 12 GHz Absorption Range
    • 100:4.3 Controlled Mixing
    • Below 180 deg C Service Temperature
  • LAIRD CR-117

    LAIRD CR-117

    • 100:3.2 Part A:B Mixing
    • 4 to 8 GHz Grade Range
    • ECCOSORB MF-117 Cured Equivalence
  • LAIRD CR-124

    LAIRD CR-124

    • Below 5 GHz Absorption Range
    • 100:2.6 Controlled Mixing
    • Up to 150 deg C Service Temperature
  • LAIRD CRS-117

    LAIRD CRS-117

    • Flexible RTV Silicone Microwave Absorber
    • 100:1.18 Controlled Mixing
    • 0.9 W/(m K) Thermal Conductivity
  • LAIRD CRS-124

    LAIRD CRS-124

    • Flexible RTV Silicone Microwave Absorber
    • 100:1.00 Controlled Mixing
    • 1.0 W/(m K) Thermal Conductivity
  • LAIRD CRS-124CRS-124

    LAIRD CRS-124CRS-124

    • Custom Cast Microwave Loads
    • Above-1-GHz RF Attenuation
    • Impact-Resistant Silicone Elastomer

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers